Extrusion Plastometers, in laboratory plastic melted mass Flow Index Testers ISO 1133, ASTM D1238, The melt mass-flow rate (MFR) and the melt volume-flow rate (MVR);
MFI series Melt Flow Index Tester/Extrusion Plastometer.
They are suitable to measure the melt flow character of PP, PE, PVC, POM, ABS etc., plastic materials resin and granules.
Principle: The melt mass-flow rate (MFR) and the melt volume-flow rate (MVR) are determined by extruding molten material from the cylinder of a plastometer through a die of specified length and diameter under preset conditions of temperature and load.
Extrusion plastometers, also known as melt flow index testers are used to determine the melt mass flow rate (MFR) and melt volume flow rate (MVR) of a plastic melted mass. Measurement of the flow behavior of the melted material is used to compare different grades of the same polymer and provides an important parameter for quality assurance and incoming goods inspections, for material selection and the setup of processing machines by plastics processors. Demands on these melt flow indexers vary according to which plastics processing stage is involved.
Feature of MFI402:
LCD display, only MFR method, motorized cutting, with micro-printer.
Test Procedure:
Approximately 7 grams of the material is loaded into the barrel of the melt flow apparatus, which has been heated to a temperature specified for the material. A weight specified for the material is applied to a plunger and the molten material is forced through the die. A timed extrudate is collected and weighed. Melt flow rate values are calculated in g/10 min.
Specimen size:
At least 14 grams of material;
Data:
Flow rate = ( 600/t x weight of extrudate )
t = time of extrudate in seconds
melt flow rate = g/10 min.
Other name:
Melt flow index testing equipment; melting flow indexer; melt indexer iso 1133; digital melt flow rate tester; quality melt flow index testing machine; melt flow index astm; plastic Melting Flow Index tester
| Model | MFI402 (XNR-400A) |
| Temperature range | Ambient temperature to 450℃ stepless adjustable, fixed point temperature control |
| Temperature fluctuation | ±0.5℃ |
| Temperature resolution | 0.1℃ |
| Weight | 8 levels, total 21.6kg mass |
| Measuring method & range | MFR (0.1-100)g/10min |
| Heating power | 450W |
| Extruding part spec. | |
| Inner diameter of die | φ2.095±0.005mm |
| Length of die | 8.000±0.025mm |
| Inner diameter of filling canister | Φ9.550±0.025mm |
| Weight | Frame: 30kg Standard weights: 25kg |
| Power | 220V, 50HZ/110V, 60HZ |
| Display | LCD display temperature, time, sampling number etc. |
| Micro-printer | YES |
| Specimen cutting mode | Automatic |
| Other model: 1, MFI401 LCD display, economical type, manual cutting, only MFR test method; 2, MFI403 LCD display, motorized cutting, both MFR/MVR test method; | |
| Item | Quantity |
|---|---|
| Frame | 1 set |
| Die (φ2.095) tungsten carbide material | 1 pc |
| No. 1 weight (piston rod + weight tray): 325g | 1 pc |
| No. 2 weight: 875g | 1 pc |
| No. 3 weight: 1835g | 1 pc |
| No. 4 weight: 3475g | 1 pc |
| No. 5 weight: 4675g | 1 pc |
| No. 6 weight: 5000g | 1 pc |
| No. 7 weight: 2500g | 1 pc |
| No. 8 weight: 2915g | 1 pc |
| Scraper | 1 pc |
| Sample loading hopper | 1 pc |
| Water level | 1 pc |
| Die cleaning rod | 1 pc |
| Cylinder cleaning rod | 1 pc |
| Sample loading rod | 1 pc |
| Sample plate | 1 pc |
| Electric wire | 1 pc |
| Cleaning gauze and gloves | 1 pc |
| Accessories containing case | 1 pc |
| Documents (Manual, packing list, certificate) | |
ISO 1133 "Plastics - Determination of the Melt Mass-Flow Rate (MFR) and Melt Volume-Flow Rate (MVR) of Thermoplastics”
ASTM D1238 "Standard Test Method for Melt Flow Rates of Thermoplastics by Extrusion Plastometer“
ASTM D3364 (for PVC), BS 2782, DIN 53735, JIS K7210