Home >> Products >> Plastic Pipe Industry Testing >> Melt Flow Index test >> Plastic Melt Flow Index Meter
Plastic Melt Flow Index Meter

Plastic Melt Flow Index Meter

Model: MFI402, Plastometer ISO 1133, MFI test MFR, MVR

MFI402 Plastic Melt Flow Index Meter is for melt mass-flow rate (MFR), determined by extruding molten material from the cylinder of a plastometer through a die of specified length and diameter under preset conditions of temperature and load. Used to measure the melt mass flow rate of thermoplastic plastics under specific temperatures and pressures, reflecting the flow performance of materials through standardized testing. 


Feature of MFI402:

LCD display, Economical price, MFR method, motorized cutting, with micro-printer.

General introduction

MFI402 Plastic Melt Flow Index Meter is for melt mass-flow rate (MFR), determined by extruding molten material from the cylinder of a plastometer through a die of specified length and diameter under preset conditions of temperature and load. Used to measure the melt mass flow rate of thermoplastic plastics under specific temperatures and pressures, reflecting the flow performance of materials through standardized testing. 


Feature of MFI402:

LCD display, Economical price, MFR method, motorized cutting, with micro-printer.


There are two main procedures:

Procedure A (for MFR): This involves manually cutting and weighing the extruded plastic at timed intervals.

Procedure B (for MVR): Instead of weighing, this method tracks how far the piston moves using displacement sensors, giving you volume flow.

Accuracy is everything in these tests. Small changes in temperature, load, or die size can skew the results. That’s why standardized test conditions—like those in ASTM D1238 or ISO 1133—are followed strictly.

Model MFI402 is for only MFR, so deduct the related parts with MVR and reduced the cost. 


Main Features

  • Key feature
  • Test Procedure
  • Standard

Mainframe is desk-top model, with beautiful appearance and stable performance, high accuracy, easy to use.

With high sampling, and high control rate.

With Micro-printer to print test result.

Only remain MFR method to meet many kinds materials, reduce cost to make this model economical price and budgetary project.

Manual and motorized both way cutting sample. 

Approximately 7 grams of the material is loaded into the barrel of the melt flow apparatus, which has been heated to a temperature specified for the material. A weight specified for the material is applied to a plunger and the molten material is forced through the die. A timed extrudate is collected and weighed. Melt flow rate values are calculated in g/10 min. 

ISO 1133  Plastics - Determination of the Melt Mass-Flow Rate (MFR) and Melt Volume-Flow Rate (MVR) of Thermoplastics

ASTM D1238  Standard Test Method for Melt Flow Rates of Thermoplastics by Extrusion Plastometer


ASTM D3364 (for PVC), BS 2782, DIN 53735, JIS K7210

Main technical specification

ModelMFI402
(XNR-400A)
Temperature rangeAmbient temperature to 450℃ stepless adjustable, fixed point temperature control
Temperature fluctuation±0.5℃
Temperature resolution0.1℃
Weight8 levels, total 21.6kg mass
Measuring method & rangeMFR (0.1-100)g/10min
Heating power450W
Extruding part spec.
Inner diameter of dieφ2.095±0.005mm
Length of die8.000±0.025mm
Inner diameter of filling canisterΦ9.550±0.025mm
WeightFrame: 30kg
Standard weights: 25kg
Power220V, 50HZ/110V, 60HZ
DisplayLCD display temperature, time, sampling number etc.
Micro-printerYES
Specimen cutting modeAutomatic


Main Accessories

ItemQuantity
Frame1 set
Die (φ2.095) tungsten carbide material1 pc
No. 1 weight (piston rod + weight tray):  325g1 pc
No. 2 weight: 875g1 pc
No. 3 weight: 1835g1 pc
No. 4 weight: 3475g1 pc
No. 5 weight: 4675g1 pc
No. 6 weight: 5000g1 pc
No. 7 weight: 2500g1 pc
No. 8 weight: 2915g1 pc
Scraper1 pc
Sample loading hopper1 pc
Water level1 pc
Die cleaning rod1 pc
Cylinder cleaning rod1 pc
Sample loading rod1 pc
Sample plate1 pc
Electric wire1 pc
Cleaning gauze and gloves1 pc
Accessories containing case1 pc
Documents (Manual, packing list, certificate)


Standard

ISO 1133 Test Method of Determination melt mass-flow rate (MFR, MVR) –

ISO 1133: Plastics -- Determination of the melt mass-flow rate (MFR) and the melt volume-flow rate (MVR) of thermoplastics.

ISO 1133 standard specifies two procedures for the determination of the melt mass-flow rate (MFR) and the melt volume-flow rate (MVR) of thermoplastic materials under specified conditions of temperature and load. One is a mass-measurement method. The other is a displacement-measurement method. Normally, the test conditions for measurement of melt flow rate are specified in the material standard with a reference to ISO 1133. The test conditions normally used for thermoplastics are listed in annexes. 

ASTM D1238 Polymer Melt Flow Rate Testing by Extrusion Plastometer –

ASTM D1238 Standard Test Method for Melt Flow Rates of Thermoplastics by Extrusion Plastometer


ASTM D1238 test method test method covers the determination of the rate of extrusion of molten thermoplastic resins using an extrusion plastometer. it is particularly useful for quality control tests on thermoplastics. The data produced by ASTM D1238 test serves to indicate the uniformity of the flow rate of the polymer as made by an individual process. It is not to be used as an indication of uniformity of other properties without valid correlation with data from other tests.

ASTM D3364 Flow Rates for Poly Vinyl Chloride, PVC Melt Flow Index Test –

ASTM D3364: Standard Test Method for Flow Rates for Poly(Vinyl Chloride) with Molecular Structural Implications

ASTM D3364 test method is an extension of Test Method D1238 specific to the measurement of flow rates of poly(vinyl chloride) (PVC) compounds while detecting and controlling various polymer instabilities associated with the flow rate. it is useful for quality-control tests on PVC compounds having a wide range of melt viscosities. Measurements are made at shear rates close to 1 s−1.  

IEC 60811-4-1 Testing methods for Insulating and sheathing materials of electric and optical cables –

IEC 60811-4-1:2004 specifying five specialized test methods for polyethylene (PE) and polypropylene (PP) compounds used as insulating and sheathing materials in electric and optical fiber cables for power distribution, telecommunications, shipboard, and offshore applications. 

Test Methods specific to polyethylene and polypropylene compounds – Resistance to environmental stress cracking – Measurement of the melt flow index – Carbon black and/or mineral filler content measurement in polyethylene by direct combustion - Measurement of carbon black content by thermogravimetric analysis (TGA) – Assessment of carbon black dispersion in polyethylene using a microscope.

Frequently Asked Questions

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.