The carbon black content tester is used to measure the carbon content in PE, PP, PB etc. , sample under nitrogen condition, through high temperature pyrolysis, then measure the weight to get the carbon level. With feature of easy operation, working reliable, and result high accuracy.
Conform with standard ISO 6964. ASTM D1603 ISO 1408, IEC 60811-4-1
Main Features:
1. The instrument has beautiful appearance and structure and simple operation;
2. Integrated design of heating furnace body and control system, convenient for user instrument management.
3. High degree of automation, only need to set the temperature value and heating time, the instrument automatically heats up to the set value;
4. High temperature control accuracy, large temperature range, high furnace temperature uniformity;
5. 7 inch LCD touch screen display, extremely friendly operation interface, can be started with one button
6. It has excellent constant temperature function, and can set the constant temperature time, and the constant temperature accuracy is high;
7. The instrument can set any group of different heating time periods, and can have different heating temperature, heating rate, and constant temperature time;
8. Can test 4 samples at a time, with the sample feeding holder.
9. The parameter display is comprehensive, showing the number of setting groups, theoretical
Display mode | 7 inch capacitive touch screen |
Quartz tube size | φ44×600±5mm |
Furnace size | Φ45×300±5mm |
Heating element | superalloy wire |
Heating zone length | 250mm |
Working temperature | room temperature ~ 1150°C |
Temperature control | intelligent programmable control, can set the segmentation program |
Air path control | two ways, program automatic switching |
Data calculation | the software comes with calculation function, one-click calculation; It can automatically calculate the carbon black content and ash content |
Cooling method | rapid cooling (≤20min, 900°C to room temperature) |
Number of test samples | 4 samples at a time |
Sample feeding holder | yes |
Sensor sensitivity | 0.1℃ |
Power | 220V, 50HZ |
Customized guide rail type sample holder, easy to take and place lofts; Open lid for quick cooling; With exhaust gas filter device; With exhaust gas filter device. | |
Item | Quantity |
Heating furnace | 1 set |
Sample holder | 1 set |
Burning boat | 5 pcs |
Power wire | 1 pc |
10A Fuse | 5 pcs |
Exhaust gas filtration | 1 set |
Tool | 1 set |
Documents (Manual, packing list, certificate) | |
ISO 6964: Polyolefin pipes and fittings -- Determination of carbon black content by calcination and pyrolysis -- Test method and basic specification.
IEC 60811-4-1: INSULATING AND SHEATHING MATERIALS OF ELECTRIC AND OPTICAL CABLES - COMMON TEST METHODS - PART 4-1: METHODS SPECIFIC TO POLYETHYLENEAND POLYPROPYLENE COMPOUNDS - RESISTANCE TO ENVIRONMENTAL STRESS CRACKING - MEASUREMENT OF THE MELT FLOW INDEX - CARBON BLACK AND.
ISO 1408:1995
Rubber — Determination of carbon black content — Pyrolytic and chemical degradation methods