Carbon Black Content Tester is also named Plastic Ash Content Tester; Ash content test Polypropylene Plastic Ash Content or Carbon Black Purity Testing Machine for the determination of carbon black content in polyethylene, polypropylene and polybutene plastics.The Carbon black in plastic does not show significant enhancement effect, but it can improve its thermal deformation, dimensional stability, rigidity and hardness, etc.
Carbon Black Content Tester is used to determine carbon black content in geomembranes,Polyolefin(Polyethylene ,polypropylene and polybutene ) Pipes.
The test of carbon black is obtained through the analysis of the weight of the samples under the protection of nitrogen. The instrument has advantages of convenient operation, simple operation, accurate measurement, high precision and high automation.
With features of easy operation, working reliable, and result high accuracy.
Standard: ISO6964; IEC60811-4-1:2004; GB13021-1991; GB/T 2951.41-2008
Model | UT3500 |
Test temperature | Ambient temperature to 990℃ |
Temperature Adjusting | Full range, free setting |
Display | LCD |
Heating tube inner diameter | Dia. 31*(400+-50)mm |
Main Accessory | Heating furnace, Burning boat, Power wire, Sensor, Rubber hose (1m, 3m), Tools |
Heating furnace,
Burning boat,
Power wire,
Sensor,
Rubber hose (1m, 3m),
Tools
ISO 6964: Polyolefin pipes and fittings -- Determination of carbon black content by calcination and pyrolysis -- Test method and basic specification.
IEC 60811-4-1: INSULATING AND SHEATHING MATERIALS OF ELECTRIC AND OPTICAL CABLES - COMMON TEST METHODS - PART 4-1: METHODS SPECIFIC TO POLYETHYLENEAND POLYPROPYLENE COMPOUNDS - RESISTANCE TO ENVIRONMENTAL STRESS CRACKING - MEASUREMENT OF THE MELT FLOW INDEX - CARBON BLACK AND/