UT2048 Rubber electric cutting press is a new type of simple fast slicer, connected to 220V power supply can be realized on rubber, plastic, wire and cable, leather and other special materials cut into a variety of standard test chips for testing, but also when small punch use, changed the manual type needs to be vigorous, pneumatic type needs to have air pressure on-site limitations.

Model | UT2048 |
Cutting stroke | ≥ 100mm |
Punching force | 10KN (1 ton) |
Work table size | 250X180mm |
Power supply | 220V 50Hz |
Weight | 45kg |
Dimensions | 350X220X450mm |