Izod Impact Testing (Notched Izod) ASTM D256, ISO 180 is a common test to understand notch sensitivity in plastics. Scope: Notched Izod Impact is a single point test that measures a materials resistance to impact from a swinging pendulum.
Notched Izod Impact is a single point test that measures a materials resistance to impact from a swinging pendulum. Izod impact is defined as the kinetic energy needed to initiate fracture and continue the fracture until the specimen is broken. Izod specimens are notched to prevent deformation of the specimen upon impact. This test can be used as a quick and easy quality control check to determine if a material meets specific impact properties or to compare materials for general toughness.
United Test product both the IZOD and Charpy impact tester, in dial display, LCD screen display and computer control used determine the impact ductility of nonmetallic materials, such as Rigid thermoplastic and thermosetting plastic, thermosetting plastic and thermoplastic after fiber-reinforced. It is widely used in the industries of plastic products, plastic manufacture, petro chemical etc, University, scientific research institute and commodity inspection department.
Charpy Test: The specimen is mounted horizontally and supported unclamped at both ends. The hammer is released and allowed to strike through the specimen. If breakage does not occur, a heavier hammer is used until failure occurs.
IZOD Test: The specimen is clamped into the pendulum impact test fixture with the notched side facing the striking edge of the pendulum. The pendulum is released and allowed to strike through the specimen. If breakage does not occur, a heavier hammer is used until failure occurs. Since many materials (especially thermoplastics) exhibit lower impact strength at reduced temperatures, it is sometimes appropriate to test materials at temperatures that simulate the intended end use environment.
Feature of XJUD series LCD Display electronic IZOD impact testing machine:
1, LCD display, IZOD Test model;
2, Adopts rotate encoder grating side angle technology, high accuracy, high reliability, and big measuring range;
3, Support vice, pendulum is nickel coating, good appearance and anti-corrosion.
4, Standard ISO 180, ASTM D256.
5, Indicate impact energy, impact strength, initial angle, rising angle, energy loss etc.,
6, Automatic correcting the energy loss; Auto-print and save the records.
7, Full range XJUD-22F is available, energy range 1J, 2.75, 5.5J, 11J, 22J

Plastic V notch impact sample 80*10*4mm Organic glass V notch impact sample 80*10*4mm
Izod Impact Testing (Notched Izod) ASTM D256, ISO 180 is a common test to understand notch sensitivity in plastics. Scope: Notched Izod Impact is a single point test that measures a materials resistance to impact from a swinging pendulum.
| Model | XJUD-5.5 | XJUD-22 |
| Impact energy | 1J, 2.75, 5.5J | 5.5J, 11J, 22J |
| Impact speed | 3.5m/s | 3.5m/s |
| Pendulum initial angle | 160° | 160° |
| Free impact energy loss | Less than 0.05J | Less than 0.1J |
| Initial potential energy error | Less than±1.5% | |
| Pendulum center to impact blade distance | 322mm | 322mm |
| Distance from impact blade to upper surface | 22mm | 22mm |
| Blade angle radius | R=0.8mm | R=0.8mm |
| Power | 220V, 50HZ | |
| Display type | LCD display | |
| Specimen clamping type | IZOD | |
| Standard Accessories | Loadframe, pendulum(1J, 5.5J), pendulum weight (2.75J), vice adjusting plate, spanner, power cord, manual etc. | Loadframe, pendulum(5.5J, 11J, 22J), vice, impact standard plate, spanner, power cord, manual etc. |
Loadframe,
pendulum,
supporting vice jaws,
specimen centering plate,
spanner,
manual etc.
ISO 179: “Plastics -- Determination of Charpy impact properties”
ASTM D6110: “Standard Test Method for Determining the Charpy Impact Resistance of Notched Specimens of Plastics”
ISO 180: “Plastics -- Determination of Izod impact strength”
ASTM D256: “Standard Test Methods for Determining the Izod Pendulum Impact Resistance of Plastics”
ISO 9854: “Thermoplastics pipes for the transport of fluids -- Determination of pendulum impact strength by the Charpy method”
ISO 8256: "Plastic Stretch Impact Intensity Determination" (method A)
ASTM D1822: "Plastic And Electric insulation Material Stretch Impact Performance test Method".