UT4016A Paint Coating Tubular Impact Tester is used in the coating of lacquer film on metal substrates, designed according to GB/T1732-93, ASTM D2794. Hammers with fixed quality standards are observed at a certain height fall on the test sample, observing the maximum height that does not cause film damage, in kg.cm units.
Model | 4015A |
Ruler length | 120±0.2cm |
Scales | 1cm |
Hammer unit weight | (2000±2)g |
Impact head indenter diameter | 15.9mm |
Diameter of socket of cushion block | 16.3mm |
Radius of curvature | R2.5~3㎜ |
Impact head impact depth | 2.5±0.1㎜ |
ASTM D2794 Standard Test Method for Resistance of Organic Coatings to the Effects of Rapid Deformation (Impact)