Model: UT4015C, ASTM D2794
Paint Coating Tubular Impact Tester is used in the coating of lacquer film on metal substrates, designed according to GB/T1732-93, ASTM D2794. Hammers with fixed quality standards are observed at a certain height fall on the test sample, observing the maximum height that does not cause film damage, in kg.cm units.
General Introduction
Paint Coating Tubular Impact Tester is used in the coating of lacquer film on metal substrates, designed according to GB/T1732-93, ASTM D2794. Hammers with fixed quality standards are observed at a certain height fall on the test sample, observing the maximum height that does not cause film damage, in kg.cm units.
ASTM D2794 Standard Test Method for Resistance of Organic Coatings to the Effects of Rapid Deformation (Impact)
Main parameters
| Model | UT4015C |
| Ruler length | 120±0.2cm |
| Scales | 1cm |
| Hammer unit weight | (2000±2)g |
| Impact head indenter diameter | 15.9mm |
| Diameter of socket of cushion block | 16.3mm |
| Radius of curvature | R2.5~3mm |
| Impact head impact depth | 2.5±0.1mm |