Information on the most widely used ASTM standards within the materials testing industry
T type. Elbow type pipe fitting end cap
Pipe fitting end closure
Used to lock the pipe test sample, the end closures seal off the sample in order to generate internal pressure in the sample. Maximum pressure depends on standard, specifications and pipe sample diameter. The design of the small end closure device for small diameter and large diameter pipe samples is different from the design of medium and large end closure devices.
Main Structural Features of UnitedTest end cap:
Pipe fitting end closure
Used to lock the pipe test sample, the end closures seal off the sample in order to generate internal pressure in the sample. Maximum pressure depends on standard, specifications and pipe sample diameter. The design of the small end closure device for small diameter and large diameter pipe samples is different from the design of medium and large end closure devices.
An air release valve is used to discharge the remaining air in the pipeline. The intelligent patented design ensures quick assembly. UnitedTest end closure devices are made of 100% stainless steel AISI 304 (proof available).
Internal sealing type for the pipe fitting.
1, Annual production end closure tens of thousands sets to ensure our technical and quality of this important pipeline hydrostatic pressure test fixtures;;
2, We adopt raw material is 45# carbon steel or 304# stainless steel, several type end closures for pipe or pipe fitting;
3, ISO 1167 Type A structure, External type: for diameter 16mm till 2000mm, three to six petals structure(not welding), no leakage under high pressure, Nickle coating, reliable and durable, 100% success installation.

Material: Typically made of 304 stainless steel, which is corrosion-resistant and has high strength.
Design: The split structure facilitates installation, achieving a sealing rate of 100%, and supports quick disassembly and assembly.
Stainless Steel End Caps For Pipe Hydrostatic Pressure and Burst Testing are designed for internal hydrostatic pressure testing of pipes and fittings. It is used to seal the sample in order to generate internal pressure in the sample, with the characters: ISO 1167 Type A structure, External type: for diameter 16mm till 2000mm, three to six petals structure(not welding), no leakage under high pressure, Nickle coating, reliable and durable, 100% success installation.
Key features
304# stainless steel
Cast iron for large size.

Standard dimensions: φ16, φ20, φ25, φ32, φ40, φ50, φ63, φ75, φ90, φ110, φ125, φ140, φ160, φ180, φ200, φ225, φ250,φ280, φ315, φ355, φ400, φ450, φ500, φ560, φ630, φ710, φ800, φ900, φ1000, φ1100, φ1200, φ1400, φ1600, φ1800, φ2000.
Inch size: 1/2"
, 3/4" , 1" ,1-1/4" , 1-1/2" , 2" , 2-1/2" , 3" , 4" , 5" , 6"
, 8" , 10" , 12" , 14" , 16" , 18" , 20“, 24"
Main technical specification
Standard dimensions: φ16, φ20, φ25, φ32, φ40, φ50, φ63, φ75, φ90, φ110, φ125, φ140, φ160, φ180, φ200, φ225, φ250,φ280, φ315, φ355, φ400, φ450, φ500, φ560, φ630, φ710, φ800, φ900, φ1000, φ1100, φ1200, φ1400, φ1600, φ1800, φ2000.
Inch size: 1/2"
, 3/4" , 1" ,1-1/4" , 1-1/2" , 2" , 2-1/2" , 3" , 4" , 5" , 6"
, 8" , 10" , 12" , 14" , 16" , 18" , 20“, 24"
Material: Cast iron (for above 110mm), or 304 stainless steel .
Other name:
End cap for HDPE pipe, End closure for PVC pipe, pipe fitting etc.,
HYDROSTATIC
PRESSURE OR INTERNAL PRESSURE TEST MACHINE FOR PVC(U) AND HDPE, Plastic
Pipe Hydrostatic Pressure Testing Equipment, pipe internal pressure
testing machine; thermoplastic pipe, pipe fitting hydrostatic pressure
testing machine; internal hydrostatic pressure testing; pipe burst
pressure testing, pipe long time pressure test.
What's the End cap of pipe pressure test?
Understand the pipe end cap for hydrostatic pressure test:
The hydrostatic pressure test end cap is specialized equipment used to detect the pressure-resistant performance of pipes, primarily used for static hydraulic tests and burst tests of plastic pipes (such as PVC, PE, PPR, etc.). It conducts pressure testing by sealing the ends of the pipes to assess their long-term static hydraulic strength and pressure resistance.
Core Functions:
Sealing Test: Achieved through silicone sealing rings and radial sealing design, firmly sealing the ends of the pipes to prevent liquid leakage during testing.
Specification Compatibility: Supports various diameters (such as Φ16-Φ1600mm), suitable for testing the requirements of different materials such as PVC, PE, PPR, and composite pipes.
Compliance with Standards: Adheres to national standards such as GB/T 6111 and GB/T 15560, as well as international standards like ISO 1167.
Standard
EN 1796 Plastics piping systems for water supply with or without pressure — Glass‑reinforced thermosetting plastics (GRP) based on unsaturated polyester resin (UP)
EN 1796 is the European product/system standard for plastics piping systems for water supply with or without pressure, made from glass-reinforced thermosetting plastics (GRP) based on unsaturated polyester (UP) resin. It covers pipes, fittings (bends, branches, reducers, saddles, flanged adaptors) and joints, classifies them by DN / PN / SN, and sets the type-test (TT) and batch-release (quality-control) test scheme that a manufacturer, a certification body or a third-party laboratory must run to prove a 50-year design life for buried (and, with care, non-buried) water pipelines.
It defines material composition (E‑glass/C‑glass/R‑glass reinforcement, UP resin, elastomer gaskets), wall‑layer construction (inner liner, structural layer, outer protective layer), dimensional tolerances, marking rules, mechanical performance, long‑term creep, hydrostatic pressure resistance and full joint performance requirements.
ISO 7509 Plastics piping systems - Glass-reinforced thermosetting plastics (GRP) pipes - Determination of time to failure under sustained internal pressure
ISO 7509 specifies a laboratory method for measuring how long a GRP pipe specimen survives under a constant internal hydrostatic pressure at a controlled temperature. It is a long-term, slow-rate stress-rupture test — not a short-term burst test.
Require More Customized Solutions?