Home >> Products >> Impact Testing Machine >> Metal Impact Tester >> Computer Controlled Impact Testing Machine
Computer Controlled Impact Testing Machine

Computer Controlled Impact Testing Machine

Model: JBW-300B

JBW-B series impact tester is mainly used to determine the anti-impact capability of ferrous metal materials with high toughness, especially for steel and iron and their alloy, under dynamic load.

This series tester is operated semi-automatically, the pendulum of the machine can be raised or released automatically. Be applicable for continuing testing in different kinds of laboratories and other metallurgy industrial manufactories.

It is designed and developed according to standard of ISO 148-1, ASTM E23, EN 10045-1, JIS Z 2242, AASHTO T 266 etc.,

General Introduction

JBW-B series impact tester is mainly used to determine the anti-impact capability of ferrous metal materials with high toughness, especially for steel and iron and their alloy, under dynamic load.

This series tester is operated semi-automatically, the pendulum of the machine can be raised or released automatically. Be applicable for continuing testing in different kinds of laboratories and other metallurgy industrial manufactories.

It is designed and developed according to standard of ISO 148-1, ASTM E23, EN 10045-1, JIS Z 2242, AASHTO T 266 etc.,


Computer Controlled Impact Testing Machine


According to ISO 148, standard specimen sizes are 10 mm × 10 mm × 55 mm. Subsize specimens are: 10 mm × 7.5 mm × 55 mm, 10 mm × 5 mm × 55 mm and 10 mm × 2.5 mm × 55mm.


ASTM E23 “Standard Test Methods for Notched Bar Impact Testing of Metallic Materials”

ISO 148 “Metallic materials -- Charpy pendulum impact test”

BS EN 10045-1 “Charpy impact test on metallic materials. Test method (V- and U-notches)” 

GOST 9454 “Metals. Method for testing the impact strength at the low, room and high temperature”

Key Features

  • Features
  • Software Introduction

1), Pendulum rising, impact, free releasing etc. action can be controlled easily by PC mouse simple click, as well as the remote control box;

2), Safety pin guaranties the impact action, standard protection shell to avoid any accident 

3), With two pendulums (big and small), digital display the energy loss, impact tenacity, rising angle, and test average value, meantime the dial scale show test result as well.

4), With two pendulums (big and small), PC software to display the energy loss, impact tenacity, rising angle, test average value etc. test data and result, also the curve display available; with calculation and report printing function. The dial scale can show test results too.

1, Windows version XP,Vista,7, 10, screen display, operation with Mouse & Keyboard;

2, Test result can export to MS Word, (2010, 2017), does not support MS Office Home Edition;

3, The software support two or more  pendulums in a model, set the accurate Local Accelaration due to gravity, fall angle, pendulum length,pendulum mass or weight,to obtain a more accurate test performance;

4, Support Min,Max,Mean,Standard Deviation for batch test;

5, High precision swing period auto-detection;

6, High precision energy loss auto-detection,auto-compensation;


Computer Controlled Impact Testing Machine

Main interface


Computer Controlled Impact Testing Machine

Specimen Information Creating


Computer Controlled Impact Testing Machine

Swing Period Detect


Computer Controlled Impact Testing Machine

System parameter


Computer Controlled Impact Testing Machine

Language selection

Main Technical Specification

Model

JBW-300B 

(JBW-300Z)

JBW-500B

(JBW-500Z)

JBW-750B

(JBW-750Z)

Display modeComputer
Impact energy300J/150J500J/250J750J
Distance between   pendulum center to impact point750mm800mm750mm
Impact   velocity5.2m/s5.4m/s5.24 m/s
Pendulum preparing angle150º
Span of specimen seat40+0.2mm
Round angle radius of GripsR1-1.5mm
Round angle radius of striking edgeR2-2.5mm, R8±0.08mm
Angle of impact knife30°
Specimen size10 (7.5, 5,   2.5)mm*10mm*55mm
Power supply3 phases 4 lines,   50Hz, 380V
Weight600Kg900Kg2500Kg
*** JBW-Z series is fully automatic,   with automatic sample feeding system.


Main Accessories

High Stiffness Frame1 set
Large pendulum 300J/500J1 set
Small pendulum 150J/250J1 set
Motor (on the loadframe)1 set
Rising pendulum driving device (on the loadframe)1 set
Automatic hitch pendulum device (on the loadframe)1 set
Safety pin (on the loadframe)1 set
Computer1 set
Printer1 set
Manual control box1 set
Supporting seat span adjusting device (L=40)1 set
Specimen center device ( L=40 V.U type)1 set
Safety cover1 set
Device to dismantle pendulum1 set
Terra anchor bolts (M16×300)1 set
Documents (Manual, packing list, certificate)


Standard

ISO 148-1 Metal Charpy pendulum impact test methods –

ISO 148-1 defines the method for the Charpy (V-notch & U-notch) pendulum impact test to determine the absorbed energy when a notched metallic specimen is broken by a single swinging pendulum blow. It does not cover instrumented impact testing (that belongs to ISO 14556). 

ISO 148-2 Verification Charpy impact testing machines –

ISO 148-2 specifically formulated for the verification, calibration and performance inspection of Charpy pendulum impact testing machines used in Charpy impact tests per ISO 148-1. 

ISO 148-3 Charpy V-notch test pieces for indirect verification of pendulum impact machines –

ISO 148-3 core focus is to establish unified rules for manufacturing, qualification, certification and proper use of Charpy V-notch reference test pieces, which are essential for the indirect verification of Charpy impact machines as required by ISO 148-2.

EN 10045-1 Charpy Impact Test for Iron and Steel Castings –

EN 10045‑1 regulates the Charpy simple-beam pendulum impact test for metallic materials, covering both V-notch and U-notch specimens. It defines unified rules for specimen preparation, machine requirements, operating conditions and result reporting.

ASTM E23 Impact Test Methods for Metal Notched Bar –

ASTM E23 covers both Charpy (simple‑beam) and Izod (cantilever‑beam) notched-bar impact tests. It applies to all metallic materials for impact tests using pendulum machines.

ASTM E2248, ISO 148-4 Charpy Impact Testing of small specimen –

ASTM E2248 and ISO 148-4 governs impact tests using fully miniaturized Charpy V-notch (MCVN) specimens, where all linear dimensions (length, cross-section, ligament) are proportionally reduced. It is clearly differentiated from subsize specimens specified in ASTM E23: subsize specimens retain standard length, notch geometry and surface finish while only reducing thickness, whereas MCVN specimens shrink the entire structure to maximize test quantity from limited material. 

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.