Information on the most widely used ASTM standards within the materials testing industry
Model: UT2108GA; ISO 5636-5,ASTM D737, TAPPI T460, ASTM D726
The Gurley gas permeability tester — also called a Gurley densometer, Gurley air permeance tester, Gurley air resistance tester — measures how long a fixed volume of air takes to pass through a clamped sheet under a low, constant pressure. It is the reference instrument for ISO 5636-5 Gurley air permeance, TAPPI T460 air resistance and Gurley seconds (s/100 mL). This page explains the standards, features, test procedure, related fixtures, applications and FAQ, and shows how UnitedTest, a professional manufacturer of material testing machines, supports both Gurley testing and ASTM D737 textile air permeability testing.
What Is a Gurley Gas Permeability Tester / Gurley Densometer?
A Gurley gas permeability tester is a low-pressure, fixed-volume air-flow instrument. A weighted inner cylinder floats in an outer cylinder partially filled with sealing oil; the cylinder's weight creates a mean pressure difference of approximately 1.22 kPa. Air displaced by the descending cylinder is forced through a specimen clamped over a circular orifice. The operator — or an electronic timer — records the time for 100 mL of air, normally read as two consecutive 50 mL graduations.
The result is reported two ways:
Air resistance (Gurley) — the time t in Gurley seconds, i.e. s/100 mL. Higher seconds mean a denser, less permeable sheet; lower seconds mean a more open, porous sheet.
Air permeance — the normalized flow property in µm/(Pa·s), where 1 ml/(m²·Pa·s) = 1 µm/(Pa·s).
General introduction
UT2108GA Air Permeability Tester is suitable for testing materials with high air permeability, such as polymer materials, battery separators, paper, films, polyurethane foam, PVC, leather, textiles, non-woven fabrics, porous ceramics, porous metals, and more, for both air permeability and air resistance. Additionally, it can be used for testing the air permeability of separation membranes, sponges, carpets, non-woven fabrics, leather, porous ceramics, and porous metals. By measuring these, it helps control material performance to meet the actual needs of the product.
The core is constant pressure, fixed volume, and timing, using the weight of the inner cylinder to create a stable pressure difference.

The Gurley Gas Permeability Tester, also known as the Gurley densometer or Gurley air resistance tester, is a precision laboratory instrument designed to measure the air permeability and air resistance of porous sheet materials. Operating on the classic Gurley method principle, this testing machine quantifies how readily air passes through a material sample under controlled pressure conditions, with results expressed in Gurley seconds — the time required for a fixed volume of air to permeate through a standardized test area.
UnitedTest, as a professional manufacturer of material testing equipment, delivers high-precision Gurley permeability testers engineered to meet the strictest international standards including ASTM D737, ISO 5636-5, TAPPI T460, and ASTM D726. Our instruments serve quality control and R&D laboratories across paper manufacturing, textile production, nonwoven fabrics, filtration media, battery separator membranes, and medical packaging industries worldwide.
Key Features
The Gurley method operates on a simple yet highly reliable gravity-displacement principle:
A precision-machined inner cylinder of known weight floats vertically within an outer cylinder partially filled with sealing oil.
The oil creates an airtight seal between the two cylinders while allowing friction-free vertical movement.
The weight of the inner cylinder generates a constant air pressure on the sample material clamped over the test orifice below.
As the inner cylinder descends under gravity, air is forced through the porous sample.
The elapsed time for a specific volume of air (typically 100 mL or 300 mL) to pass through the sample is measured — this time value, in seconds, is the Gurley air resistance value.
Air permeance is then calculated from the measured time, test area, pressure, and air volume parameters.
Gravity-driven constant-pressure system: The weighted inner cylinder floats freely in a sealing oil bath, delivering stable and repeatable test pressure of 1.22 kPa (4.88 inches water column) without requiring external compressed air supply.
Interchangeable test area orifices: Standard 1.0 in² (645 mm²) test head, with optional 0.25 in² and 0.1 in² orifice plates to accommodate materials ranging from high-porosity tissue paper to low-permeability coated barrier films.
Precision volumetric cylinder: Calibrated stainless-steel inner cylinder with engraved dual-scale graduations (25 mL initial increment, followed by 50 mL steps up to 300 mL) for accurate visual timing.
Modular clamping assembly: Hardened steel clamping platens with precision-ground gasket surfaces ensure uniform sample compression and leak-free sealing; available in hand-tightened capstan, dead-weight lever arm, or pneumatic clamping configurations.
Wide measuring range: Air resistance measurement from 0.2 seconds to over 2000 Gurley seconds, covering medium-range permeance from 0.1 µm/(Pa·s) to 100 µm/(Pa·s) per ISO 5636-5 specification.
Digital timing upgrade option: Integrated electronic timer with automatic start/stop detection for enhanced accuracy and reduced operator error compared to manual stopwatch measurement.
No external power required for basic operation: Purely mechanical design enables reliable testing in field environments and locations without electrical infrastructure.
Calibration traceability: All instruments come with calibration certificates traceable to national metrology standards, supporting ISO 17025 laboratory accreditation requirements.
| Fixture / accessory | Function | Typical specification |
|---|---|---|
| Outer cylinder | Holds sealing oil and carries the volume scale | Graduated at 50 mL and 100 mL; TAPPI reference ~254 mm high, 82.6 mm ID |
| Floating inner cylinder | Generates constant test pressure | Open-top, free-sliding, ~567 g; ~1.22 kPa mean pressure difference |
| Upper / lower clamping plates | Hold the specimen over a concentric circular aperture | Hand screw capstan, 901 g dead-weight lever, or pneumatic clamp; 180 ± 30 N |
| Rubber sealing gasket | Prevents edge and surface leakage | ID 28.6 ± 0.1 mm, OD 35.2 ± 0.1 mm, thickness 0.7–1.0 mm, groove depth 0.45 ± 0.05 mm, 50 IRHD oil-resistant rubber |
| Sealing oil | Liquid air seal between cylinder and atmosphere | Density 860 ± 30 kg/m³, 16–19 cP at 20 °C, flash point ≥135 °C; light paraffin/spindle oil, not water |
| Interchangeable test heads / orifice plates | Adapt the instrument to different permeance ranges | 1.0 in² standard; 0.25 in² and 0.1 in² optional; high-pressure heads for dense films |
| Calibration orifice / restriction plate | Traceable verification of timing and volume | Used with ISO 5636-5 Annex A and electronic timer checks |
| Non-porous leakage-check plate | Zero-flow verification | Smooth metal foil or cellophane; max 50 mL in 5 h under TAPPI T460 |
| Sample cutter / circular die | Produce flat, repeatable specimens | 100 mm × 100 mm or ≥50 mm square; diameter larger than the gasket |
| Timer / stopwatch / electronic sensor | Record displacement time | 0.1 s resolution; digital timing attachment or mass-flow sensor |
| Pressure sensor and regulator | Stabilize and verify differential pressure | 0–2 kPa range on electronic Gurley testers, 0.01 kPa resolution |
| PC software, printer, RS232 / network interface | Data logging, audit trail, report output | Real-time curve, built-in query, micro-printer, LIMS export optional |
| High-pressure densometer attachment | Shorten test time for low-permeability materials | ~12.2 in. water column, 2.5–30 cc ti |
The Gurley gas permeability tester serves as a critical quality control tool across multiple industrial sectors:
1, Pulp and Paper Industry
Printing and writing paper porosity control for ink absorption optimization
Cigarette paper permeability testing for burn rate regulation
Tissue paper and towel air resistance measurement for softness correlation
Kraft paper and packaging board barrier verification
Coated and laminated paper barrier integrity testing
2, Textile and Nonwoven Industry
Woven and knitted fabric breathability assessment for apparel
Nonwoven fabric air permeability testing for hygiene products
Meltblown media characterization for respirator and face mask filtration
Geotextile air flow testing for civil engineering applications
Airbag fabric permeability validation for automotive safety systems
3, Filtration and Membrane Industry
Filter paper and filter media air resistance qualification
Battery separator membrane permeability testing for lithium-ion batteries\
Ultrafiltration and microfiltration membrane pore structure characterization
HEPA filter media quality control and batch consistency verification
4, Medical and Packaging Industry
Sterile medical packaging breathability testing per ISO 11607
Tyvek and porous packaging material microbial barrier correlation
Food packaging barrier coating uniformity assessment
Release liner and label facestock porosity testing
ASTM D737 — Standard Test Method for Air Permeability of Textile Fabrics
ASTM D737 is the primary international standard for measuring the air permeability of textile fabrics. It specifies testing the rate of air flow passing perpendicularly through a known area of fabric at a prescribed pressure differential of 125 Pa (0.5 inch water column). The standard applies to woven fabrics, nonwovens, airbag fabrics, blankets, napped fabrics, knitted fabrics, layered fabrics, and pile fabrics — whether untreated, sized, coated, or resin-treated. UnitedTest Gurley testers fully comply with ASTM D737 Annex A1 requirements for Gurley-method air permeability testing.
ISO 5636-5 — Paper and Board Air Permeance (Gurley Method)
ISO 5636-5:2013 defines the Gurley method for determining air permeance and air resistance of paper and board in the medium range (0.1 to 100 µm/(Pa·s)). The standard specifies the apparatus design, test procedure, calculation method, and reporting format for Gurley-type air resistance testing. It is applicable to most paper and board grades but is not recommended for rough-surfaced materials that cannot be securely clamped to prevent edge leakage.
TAPPI T460: Air resistance of paper and paperboard (Gurley method), widely used in the pulp and paper industry
ASTM D726: Standard test method for air resistance of nonporous paper
ISO 9237: Textile fabrics — Determination of air permeability
GB/T 5453: Chinese national standard for textile air permeability testing
TAPPI T536: High-pressure method for low-permeability materials
JIS P 8117:2009: Paper and board — air permeance and air resistance (medium range) — Gurley method
GB/T 458-2008: Paper and board — Determination of air permeance (Gurley, Schopper, Bendtsen methods)
GB/T 36363-2018: Polyolefin separators for lithium-ion batteries
(Different principle: constant-pressure airflow through textiles, typically 125 Pa and 38.3 cm², reported in cm³/s/cm² or ft³/min/ft². See the comparison below.)
ISO 9073-15: Textile and nonwoven air permeability
ISO 5636-3 / -4 / -6 Bendtsen, Sheffield and Oken methods
Sample preparation: Cut specimens to appropriate size (minimum 50 mm × 50 mm). Condition samples in standard testing atmosphere (23°C ± 1°C, 50% ± 2% RH for paper; 21°C ± 1°C, 65% ± 2% RH for textiles) for at least 24 hours.
Instrument setup: Place the tester on a level, vibration-free surface. Fill the outer cylinder with specified sealing oil to the indicated level. Verify the inner cylinder moves freely without friction.
Orifice selection: Install the appropriate orifice plate based on expected permeability; use 1.0 in² for most standard materials, smaller orifices for high-resistance samples.
Sample clamping: Place the specimen flat over the test orifice, ensuring complete coverage. Tighten the clamping mechanism uniformly to achieve a leak-free seal without distorting the sample structure.
Test execution: Raise the inner cylinder to the starting position and engage the release catch. Start timing when the first graduation mark aligns with the outer cylinder rim. Stop timing when the target volume mark passes the reference point.
Data recording: Record the elapsed time in seconds. Test at least five specimens per sample, testing both top-side and wire-side orientations for paper materials.
Calculation: Compute the mean air resistance value. Convert to air permeance in µm/(Pa·s) using the standard conversion formula if required.
1. Conversion Principle: The core indicator of Gurley is the time it takes for 100 mL of gas to pass through the sample.
The high-precision flow meter collects the instantaneous gas flow Q (mL/s) in real time and accumulates the ventilated volume. When the accumulated gas reaches 100 mL, the time t is recorded, directly equivalent to the Gurley second value; it can also be reverse-calculated using the average flow. The supporting pressure-stabilizing system maintains the pressure difference on both sides of the sample consistent with the standard Gurley 1.23 kPa, making the test conditions equivalent (conforming) to national standards.
2. Core Advantages Compared to the Traditional Gravity Inner and Outer Bucket Method
• Good pressure difference stability: Gravity buckets rely on their weight to apply pressure, causing slight fluctuations during the descent. Flow meters with a closed-loop pressure system maintain a stable pressure difference throughout, closely matching the standard rated value and providing higher test repeatability.
• Wider range compatibility: Gravity buckets are limited by cylinder stroke and weight, restricting tests on materials with high or low permeability. Flow meters cover a wide flow range and can universally handle soft leather, films, paper, and nonwoven fabrics.
• No mechanical wear or media loss: Eliminates sealing oil and sliding cylinder structures, avoiding oil evaporation, leakage, and cylinder wall friction issues. Equipment lifespan is longer with lower maintenance costs.
• Higher data acquisition accuracy: Flow meters measure in milliseconds in real time, avoiding manual reading and visual scale errors. Timing and volume measurement accuracy far exceed mechanical readings.
• Higher testing automation: Automatic start/stop, automatic detection at the 100 mL point, and automatic Gurley time calculation—all without manual monitoring, greatly improving batch testing efficiency.
• Strong controllability of test conditions: Pressure control and airflow direction can replicate standard test environments or vary the pressure difference for extended testing, providing better compatibility.
• Simple structure with low failure rate: Eliminates reciprocating mechanical parts, reducing issues like jamming, air leaks, or weight deviation, ensuring more stable equipment performance.
• Traceable and storable data: Original flow curves and timing data are automatically saved, facilitating quality checks and dispute reviews, meeting laboratory compliance requirements.
• More stable pneumatic fixture: Cylinder pressing ensures consistent clamping force each time without human intervention.
Gurley gas permeability tester, Gurley air permeance tester, Gurley densometer, Gurley air resistance tester, ISO 5636-5 Gurley method, ASTM D737 air permeability tester, UnitedTest Gurley tester, Gurley method air resistance tester, ASTM D737 air permeability tester, ISO 5636-5 Gurley tester, TAPPI T460 paper testing machine, air permeability testing equipment, paper air permeance tester, textile air permeability test instrument, nonwoven fabric Gurley tester, battery separator permeability test, filter media air resistance tester, Gurley test orifice plate, Gurley sealing oil, UnitedTest permeability tester manufacturer, automatic Gurley air permeability tester, manual Gurley densometer, Gurley seconds measurement, porous material air permeability testing machine
Main Technical Specification
| Measurement range | 0.01-25um/(Pa.s), large ranges can be customized |
| Resolution | 0.001um/(Pa.s) |
| Permeation rate | 0.01-200ml/min (other ranges optional) |
| Pressure difference/range | 0-3KPa, accuracy: ±0.01kPa (other ranges optional) |
| Effective pressure difference Gurley method | 1.23kPa ±0.01kPa |
| Bendtsen method | 1.47kPa ±0.02kPa |
| Sheffield method | 1.00 kPa ±0.01kPa or 2.50 ±0.01kPa (airflow less than 0.13ml/L) |
| Test area (customizable) | Bendtsen method: 50mm × 50mm, effective area: 10.0 ±0.2cm2; Sheffield method: 60mm × 100mm, effective area: 10.0 ±0.2cm2; Gurley method: 50mm × 50mm, effective area: 6.42cm2. |
| Test time | 1-999999 seconds, accuracy: 0.1 seconds |
| Sample temperature and humidity treatment | A. Pre-treatment: Keep in atmospheric conditions of <40°C, 10-35% RH, and let it sit for 24 hours B. The difference in weight before and after 1 hour should not exceed 0.25% of the total mass, samples in balance. |
| Power | 220V, 50Hz/110V, 60HZ, single phase |
| Standard configuration | Main unit, one set of clamps, Φ8mm polyurethane tube |
| Key feature | Two measurement modes, constant pressure difference and constant flow (Bendtsen and Sheffield methods), customizableProfessional sample clamps for safer operation. Computer-controlled, with more powerful curve and data processing functions Win10 system, supports Bluetooth and WiFi, Office report processing, can connect to all types of printers, and results can be saved long-term. |
Standard
ISO 15105-1 Plastics — Film and Sheeting — Determination of Gas-transmission Rate — Part 1: Differential-pressure Methods
ISO 15105-1 defines two standardized differential-pressure test methods to quantify the gas barrier performance of plastic films, sheets and multi-layer plastic structures, focusing on measuring Gas Transmission Rate (GTR) and Gas Permeability Coefficient (P) under a controlled gas partial pressure difference across the specimen.
ISO 2556 Plastics — Determination of the gas transmission rate of films and thin sheets under atmospheric pressure — Manometric method
ISO 2556 defines a single mercury-based manometric differential-pressure test method to measure Gas Transmission Rate (GTR) of thin plastic films and sheets, with a measurable range of 1 to 20000 cm³/(m²·d·atm). It uses a mercury capillary manometer to quantify pressure rise in the evacuated low-pressure chamber under a fixed upstream atmospheric test gas pressure.
ASTM D1434 Standard Test Method for Determining Gas Permeability Characteristics of Plastic Film and Sheeting
ASTM D1434 defines an electronic manometric differential-pressure method to measure three core barrier metrics: Gas Transmission Rate (GTR), permeance, and material permeability (only valid for homogeneous plastics). It covers plastic films, sheets, multi-layer laminates, plastic-coated paper and plastic-coated fabrics, and follows WTO TBT international standardization principles.
ISO 2782-1 Rubber, vulcanized or thermoplastic — Determination of permeability to gases — Part 1: Differential-pressure methods.
ISO 2782-1 establishes three distinct differential-pressure test procedures exclusively for vulcanized and thermoplastic rubbers with hardness ≥35 IRHD, to quantify gas permeation performance under controlled partial pressure differences. It supports single pure gases and mixed gas blends, and delivers four core permeation parameters for rubber material characterization.
ISO 13636 specifies requirements anf test methods for non-oriented PET (APET) sheets — made from virgin, recycled, or combined PET, thickness < 2.0 mm. It explicitly excludes foamed sheets and shrinkable films (those are covered elsewhere, e.g. biaxially oriented PET in ISO 15988). The mandatory performance tests including Tensile stress at yield, Heat shrinkage, Oxygen transmission rate (OTR), haze value, Intrinsic viscosity (IV).
ISO 15988 specifies requirements for biaxially oriented transparent PET (BOPET) films, mainly used for packaging, either alone or as a laminated layer with other films. The main test stipualted in this standard include tensile strength and strain, Dimensional change on heating, Oxygen transmission coefficient, Water vapour transmission coefficient, Haze, Wetting tension, thickness etc.,
ISO 15987 specifies classification, mandatory visual, dimensional, mechanical, barrier, optical, surface energy, and food contact safety requirements for transparent BOPA film, supplied in roll form, either used standalone or laminated with PE, CPP, PET, aluminium foil for multi-layer packaging structures. The test stipulated in ISO 15987 mainly include, tensile strength & tensile strain at break, Oxygen transmission coefficient, Dimensional change on heating, Haze, Wetting tension etc.,
ISO 17555 applies to packaging-grade BOPP films containing ≥95% polypropylene resin; usable as single-layer film or laminates paired with other plastic substrates. The test stipulated in ISO 17555 mainly include, tensile strength & strain at break, Dimensional change on heating (thermal shrinkage), Coefficient of water vapour transmission, Haze, Wetting tension etc.,
Frequently Asked Questions (FAQ)
A: Gurley seconds measure air resistance — the time required for 100 mL of air to pass through a 1.0 in² sample area under standard pressure. Air permeance, expressed in µm/(Pa·s) or L/(m²·s·Pa), is the inverse measure of how easily air flows through the material. Lower Gurley seconds mean higher permeability. Standard conversion formulas are defined in ISO 5636-5.
A: Yes, UnitedTest Gurley permeability testers are versatile instruments suitable for both paper and textile materials. Paper testing generally follows ISO 5636-5 / TAPPI T460 protocols, while textile testing references ASTM D737. The difference lies primarily in test pressure, sample conditioning, and reporting units — all achievable with the same base instrument using appropriate accessories.
A: We recommend annual calibration for routine QC environments, and semi-annual calibration for laboratories operating under ISO 17025 accreditation. Calibration verification includes cylinder weight inspection, orifice area measurement, timing system accuracy, and cross-reference with certified standard reference materials.
A: Common sources of variability include: insufficient sample conditioning (temperature/humidity), uneven clamping force causing edge leakage, contaminated or worn sealing oil, misaligned cylinders causing friction, operator timing error, and testing on non-homogeneous material areas. UnitedTest digital timing systems and pneumatic clamping significantly reduce operator-dependent variability.
A: The standard Gurley method works best for medium-range permeance (0.1–100 µm/(Pa·s)). For highly porous materials like thick nonwovens or foams, test times become too short (< 2 seconds) for accurate manual measurement. In such cases, use the lightweight 5 oz cylinder option, or consider our differential-pressure air permeability tester for high-permeability ranges.
A: All three measure paper air permeability but use different pressure levels and test geometries. Gurley uses low pressure (1.22 kPa) and measures time for fixed volume — ideal for medium-to-low permeability papers. Bendtsen and Sheffield methods use higher flow rates and measure air flow at fixed pressure, better suited for more porous materials. Results are not directly convertible but show general correlation within specific material ranges.
A: Yes, UnitedTest maintains full inventory of genuine replacement parts including inner cylinders, sealing gaskets, orifice plates, sealing oil, and timing components. Most standard spare parts ship within 48 hours worldwide.
A: Absolutely. We offer custom orifice sizes, specialized cylinder weights, modified sample holders for irregular specimens, and software integration for automated testing lines. Contact our engineering team with your specific application requirements.
Require More Customized Solutions?