ASTM C473, ISO 6308
This equipment is widely used in gypsum board manufacturing enterprises, quality inspection institutions, and research units, ensuring that products meet national standards and industry regulations.
General introduction
Gypsum board bending strength testing is specifically designed to test the mechanical properties of gypsum boards under bending loads. It is mainly used to evaluate the bending strength, elastic modulus, and fracture properties of gypsum boards.
2, Main Functions:
Measures the maximum load capacity of gypsum boards in a bent state (unit: MPa).
Elastic modulus calculation: Calculates the stiffness of the material through the stress-strain curve (unit: GPa).Accordind standard the fixure span is 40 times the thickness of the Gypsum panel.