Water cooling Rotary Xenon Arc Solar Radiation Aging Testing Chamber

Water cooling Rotary Xenon Arc Solar Radiation Aging Testing Chamber

Model: UT2068R; ASTM D4459, ASTM D4355

Water cooling Rotary Xenon Arc Aging Test Chamber simulate the full sunlight spectrum to reproduce destructive light waves in different environments can provide corresponding environmental simulation and accelerated tests for scientific research, product development and quality control.


Lightfastness and weather resistance of certain materials under the action. Mainly used in automobiles, coatings, rubber, plastics, pigments, adhesives, fabrics, aerospace, ships, electronics industry, packaging industry, etc.


This xenon lamp weathering test chamber can be used for the selection of new materials, the change of existing materials or the evaluation of durability changes after the change of material composition, which can well simulate the changes caused by the exposure of materials to sunlight under different environmental conditions. 


General Introduction

Water cooling Rotary Xenon Arc Aging Test Chamber simulate the full sunlight spectrum to reproduce destructive light waves in different environments can provide corresponding environmental simulation and accelerated tests for scientific research, product development and quality control.


Lightfastness and weather resistance of certain materials under the action. Mainly used in automobiles, coatings, rubber, plastics, pigments, adhesives, fabrics, aerospace, ships, electronics industry, packaging industry, etc.


This xenon lamp weathering test chamber can be used for the selection of new materials, the change of existing materials or the evaluation of durability changes after the change of material composition, which can well simulate the changes caused by the exposure of materials to sunlight under different environmental conditions. 

Key Features

  • Standard

ASTM D2565, 

ASTM D4355, 

ASTM D4459

ISO 4892-2,

ISO 11341

ISO 16474, 

 IEC 60068-2-5

SAE J 2412, 

SAE J 2527

Main Technical Specification

Inner box size800*800*800mm(W*D*H)
Outer carton sizeApprox. 1410*1310*2000 mm (W*D*H)
Temperature rangeRT+10℃~80℃
Temperature uniformity±3℃
Temperature accuracy±0.1℃
Humidity rangeOptical   cycle: 35%~~75%RH; Dark circulation: 45~~95%RH
Humidity accuracy±1%RH
Temperature and humidity sensorsPlatinum resistors. PT100Ω/MV
Xenon range0.5W~800W/㎡ adjustable
Spectral wavelength280nm~800nm
Turntable speed1~7r/min
Turntable diameterΦ400mm
Number of lamps1 stick
Lamp lifeAbout 1~1200 hours
Xenon lamp power2.5KW(2500cm²)
Blackboard temperature40°C~~110°C±3°C adjustable
The distance from the center of the arc to the specimen250~300mm, effective exposure area 3760cm2
Filter typeSolar filter or window glass filter (optional)
Light cycle time0~999H, M, S continuously adjustable
Rainfall time0~9999min continuous rainfall can be adjusted
Rainfall cycles1~240min interval (intermittent) rainfall can be adjusted
Water spray cycleSpray 18min/stop 102min, spray 12min/stop 48min
Rainwater pressure0.12~0.15Mpa
Nozzle apertureФ0.8mm
controllerProgrammable touchscreen controller
Standard sample size75mm×150mm
Blackboard thermometerBlackplate thermometer BPT or black standard thermometer BST
Cooling methodChiller cooling (standard with one chiller)
Water quality requirementsWith pure water or deionized water, the user's laboratory needs to provide pure water   channel (pure water system optional)
Sample holder materialSUS304 high-quality stainless steel
Inner box materialSUS304 stainless steel plate
Outer box materialBaking lacquer
doorframeHigh and low temperature aging resistant silicone rubber door seal




Main Accessories


Name
SpecMark
1controller

2Fans90WTaiwan
3Heating wire2KW
4Over-temperature protectionEGOKorea
5Humidification tube
Taiwan
6Xenon lamp2.5KW
7Xenon lamp power supply2000W-2500W
8DC switch24V
9Exhaust fan220V  180W
12Turntable motor

11Leakage main switch2P  32ASchneider
12sensor
import
13AC contactors
Schneider
14compressor6PPanasonic of Japan
15Intermediate relays14 pinSchneider
16water pump
Domestic
17evaporator
Taiwan
18condenser
Taiwan
19Filter driers
Danfoss
20Refrigeration solenoid valves
Castard
21Plastic floats90°


Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.