ISO 14126
In-Plane Compressive test fixture of Fiber-Reinforced Plastic Composites
conform with ISO 14126 test standard, determining the in-plane
compression strength properties of fiber-reinforced plastic composites.
UnitedTest Supply the suitable testing machine and ISO 14126 In-Plane Compressive test fixture.
This standard describes two different methods for evaluating performance:
Method 1: Provide the shear load of the specimen
Method 2: Provide end loading or mixed loading of the sample
General introduction
Therefore, suitable extensometers or adhesive resistance strain gauges are required to measure axial strain throughout the entire testing process.