Home >> Products >> Compression Testing Machine >> Compression Test >> Large capacity compression testing machine
Large capacity compression testing machine

Large capacity compression testing machine

Model: YAW-2000 / 3000

YAW series Compressive Strength Testing Equipment to test cement, brick and concrete is offered by United Test. Range 1000KN, 2000KN, and 3000KN, these strength testing equipment are extremely handy and are easy to use for testing cement, concrete and mortar cubes. We lay utmost importance on equipment design and construct with emphasis on ease of operation.
 
Conform with test standard ASTM C39, this test method consists of applying a compressive axial load to molded cylinders or cores at a rate which is within a prescribed range until failure occurs. The compressive strength of the specimen is calculated by dividing the maximum load attained during the test by the cross-sectional area of the specimen.

General Introduction

YAW series Compressive Strength Testing Equipment to test cement, brick and concrete is offered by United Test. Range 1000KN, 2000KN, and 3000KN, these strength testing equipment are extremely handy and are easy to use for testing cement, concrete and mortar cubes. We lay utmost importance on equipment design and construct with emphasis on ease of operation.
 
Conform with test standard ASTM C39, this test method consists of applying a compressive axial load to molded cylinders or cores at a rate which is within a prescribed range until failure occurs. The compressive strength of the specimen is calculated by dividing the maximum load attained during the test by the cross-sectional area of the specimen.



Key Features

  • Features
  • Measuring and control system
  • Key part
  • Standard

Industry computer, easy operation and solid panel (class IP65), anti-shock, rustproof etc., function. 


Unitary oil source cabinet, consist of hydraulic pump, oil control & measuring system, computer etc., internal radial plunger pump output stable and low noise. High integration oil source cabinet, easy operation and observation.


Key part like upper and lower compression platen, columns, position pin hardness above 55HRC.  Surface hard chrome coating ensure the surface smooth and clean, with high anti-abrasion ability and low noise. Can work long life without lubricant oil.

Measuring and control system include digital servo valve, high accuracy load cell, controller, software, with high stability. Meet the test requirement for cement, concrete of various standard. Function of load close loop control; realize consistent speed control or consistent load control. Computer automatic complete the test, automatic calculate the test result, and print test report. 

1, The tester mainly consist oil cylinder, piston, load cell, compression platen, columns, upper crosshead, oil tank, valve manifold group, controller etc.,

2, Use load cell to measure the force, with high accuracy and good stability, repeatability.

Large capacity compression testing machine

3, Column surface chrome coating, rust protect and more beautiful appearance.
4, Running noise lower than 60dB.

ASTM C39 "Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens“
GB/T 17671, GB/T 50081, GB/T2611, GB/T16826 etc.,

Main Technical Specification

ModelYAW-2000YAW-3000
Max. load2000KN3000KN
Accuracy of testing force±1% of indicated value
Load resolution0.01kN
Frame structure4 columns frame
Upper compression platen dia.Φ300mm
Piston moving speed0-60mm/min
Distance between two platens360mm
Columns effective intervals400×320mm
Piston stroke200mm
Power supply220V, 50HZ, 1 phase
Dimension of frame640×560×1500mm700×580×1650mm
Dimension of oil source cabinet700×540×1500mm
Weight1500Kg2100Kg
Standard AccessoriesLoadframe, load cell, industry computer, compression platen, close loop controller, Software, unitary oil source cabinet, English operation manual


Main Accessories

Loadframe,
load cell,
industry computer,
compression platen,
close loop controller,
Software,
unitary oil source cabinet,
English operation manual

Standard

ISO 1920-4 Hardened Concrete Strength Test - Compressive, Flexural & Tensile Splitting –

ISO 1920-4 Testing of concrete — Part 4: Strength of hardened concrete

ISO 1920‑4 measuring mechanical strength of hardened concrete. It consolidates three core strength‑testing procedures: compressive strength, flexural strength, and tensile splitting strength of hardened concrete. covers specimens, apparatus, testing procedures, calculation formulas, failure assessment, precision data and complete test‑report requirements. 

ISO 4012 Concrete Compression Testing - Cube, Cylinder & Prism –

ISO 4012 Concrete‑Determination of compressive strength of test specimens

ISO 4012 define method for crushing hardened concrete specimens in uniaxial compression and calculating strength from maximum load divided by loaded area. it was replaced by ISO 1920‑4.

ASTM C39 Compressive Strength Test of Cylindrical Concrete Specimens –

ASTM C39 / C39M : Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens

ASTM C39 determines the compressive strength of cylindrical concrete specimens such as molded cylinders and drilled cores. It is limited to concrete having a unit weight in excess of 50 lb/ft3 (800 kg/m3).
A compressive axial load is applied to molded cylinders or cores until failure occurs. The compressive strength of the specimen is calculated by dividing the maximum load achieved during the test by the cross-sectional area of the specimen. The results of this test method are used as a basis for quality control of concrete.

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.