Model: YAW-300
YAW series Hydraulic Compression Strength Testing Machine to test cement, brick and concrete is offered by United Test. Use hydraulic power driving, hydraulic servo control technology, computer to collect and process data, close loop test with high accuracy for various test materials. Consist of frame, oil source, control system, test fixture. Accuracy class 1, max. test load 300KN.
General Introduction
YAW series Hydraulic Compression Strength Testing Machine to test cement, brick and concrete is offered by United Test. Use hydraulic power driving, hydraulic servo control technology, computer to collect and process data, close loop test with high accuracy for various test materials. Consist of frame, oil source, control system, test fixture. Accuracy class 1, max. test load 300KN.
Key Features
1, The tester mainly consist oil cylinder, piston, load cell, compression platen, columns, upper crosshead, oil tank, valve manifold group, controller etc.,
2, Use load cell to measure the force, with high accuracy and good stability, repeatability.

3, Column surface chrome coating, rust protect and more beautiful appearance.
4, Running noise lower than 60dB.
Industry computer, easy operation and solid panel (class IP65), anti-shock, rustproof etc., function.

Special design oil system pressure less than 25Mpa, ensure the security and enlarge the working life.
Key part like upper and lower compression platen, columns, position pin hardness above 55HRC. Surface hard chrome coating ensure the surface smooth and clean, with high anti-abrasion ability and low noise. Can work long life without lubricant oil.
Measuring and control system include digital servo valve, high accuracy load cell, controller, software, with high stability. Meet the test requirement for cement, concrete of various standard. Function of load close loop control; realize consistent speed control or consistent load control. Computer automatic complete the test, automatic calculate the test result, and print test report.
ISO 679:2009 "Cement -- Test methods -- Determination of strength"
GB/T 17671
Main Technical Specification
| Model | YAW-300 |
| Max. load | 300KN |
| Accuracy of testing force | ±1% of indicated value |
| Max. compress test space | 180mm |
| Upper Compression platen dia. | (Fixed type plate) Φ108mm |
| Upper Compression platen dia. | (Cardan joint type) Φ170mm |
| Lower Compression platen dia. | Φ205mm |
| Piston stroke | 80mm |
| Power supply | 220V, 50HZ, 1 phase |
| Dimension | 930×550×1400mm |
| Weight | 450Kg |
| Power | 0.75kW(Pump power 0.55 kW) |
| Standard Accessories | Loadframe, computer, English compression test software, load cell, compression platen, Safety net cover, English operation manual |
Main Accessories
Loadframe,
computer,
English compression test software,
load cell,
compression platen,
Safety net cover,
English operation manual
Standard
ISO 1920-4 Testing of concrete — Part 4: Strength of hardened concrete
ISO 1920‑4 measuring mechanical strength of hardened concrete. It consolidates three core strength‑testing procedures: compressive strength, flexural strength, and tensile splitting strength of hardened concrete. covers specimens, apparatus, testing procedures, calculation formulas, failure assessment, precision data and complete test‑report requirements.
ISO 4012 Concrete‑Determination of compressive strength of test specimens
ISO 4012 define method for crushing hardened concrete specimens in uniaxial compression and calculating strength from maximum load divided by loaded area. it was replaced by ISO 1920‑4.
ASTM C39 / C39M : Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens
ASTM C39 determines the compressive strength of cylindrical concrete specimens such as molded cylinders and drilled cores. It is limited to concrete having a unit weight in excess of 50 lb/ft3 (800 kg/m3).
A compressive axial load is applied to molded cylinders or cores until failure occurs. The compressive strength of the specimen is calculated by dividing the maximum load achieved during the test by the cross-sectional area of the specimen. The results of this test method are used as a basis for quality control of concrete.