Home >> Products >> Industrial Specialized Testing >> Civil Engineering >> Smoke Density Tester, Exit Sign Test Apparatus
Smoke Density Tester, Exit Sign Test Apparatus

Smoke Density Tester, Exit Sign Test Apparatus

Model: UT2073; ASTM D2843

The smoke density tester, also name as the Exit Sign Smoke Testing Apparatus, is a specialized device used to determine the static smoke emission of building materials and their products under combustion or decomposition conditions. It evaluates the smoke density grade of materials during combustion by measuring the loss of light flux caused by solid particles in the smoke. This instrument consists of a combustion system, a photodetection system, and a control system. It employs computer or PLC control technology to achieve automated operation, can automatically record test data, generate test reports, and plot cumulative curves of smoke density over time. It complies with the GB/T8627-2007 standard, with a measurement range of 0-100% and a measurement accuracy of ≤3% (absolute value). The combustion gas source is >95% propane, with a main burner operating pressure of 276KPa (adjustable) and an auxiliary burner pressure of 138KPa (adjustable). The diameter of the Bunsen burner nozzle is 0.13mm, and the working tilt angle is 45 degrees. 


Its technical parameters cover a smoke density measurement range of 0-100%, with an accuracy of ±3%, and comply with both domestic and international standards such as GB/T 8627-2007 and ASTM D2843.

General Introduction

The smoke density tester, also name as the Exit Sign Smoke Testing Apparatus, is a specialized device used to determine the static smoke emission of building materials and their products under combustion or decomposition conditions. It evaluates the smoke density grade of materials during combustion by measuring the loss of light flux caused by solid particles in the smoke. This instrument consists of a combustion system, a photodetection system, and a control system. It employs computer or PLC control technology to achieve automated operation, can automatically record test data, generate test reports, and plot cumulative curves of smoke density over time. It complies with the GB/T8627-2007 standard, with a measurement range of 0-100% and a measurement accuracy of ≤3% (absolute value). The combustion gas source is >95% propane, with a main burner operating pressure of 276KPa (adjustable) and an auxiliary burner pressure of 138KPa (adjustable). The diameter of the Bunsen burner nozzle is 0.13mm, and the working tilt angle is 45 degrees. 


Its technical parameters cover a smoke density measurement range of 0-100%, with an accuracy of ±3%, and comply with both domestic and international standards such as GB/T 8627-2007 and ASTM D2843.

Main features

  • Key features
  • Working Conditions
  • Instrument structure
  • Standard

1. Dual control method allows operation through the touchscreen or via a computer, with the ability to switch between modes at will.

2. One device can be operated by multiple computers simultaneously, enabling several computers to be online at the same time, allowing for LAN sharing.

3. The main and auxiliary burners can automatically rotate with precise positioning.

4. Independently developed control software can meet various operations, recording, real-time curves, and result calculations during experiments.

1. Ambient temperature: 0℃-40℃;

2. Relative humidity: ≤85%;

3. Power supply voltage and power: 220V±10%, 50HZ, 100W; 

4. Gas pressure: 0-0.3MPa (adjustable);

5. Environmental and testing requirements: Direct strong light should be avoided from shining or reflecting onto the instrument while it is working; after 90 minutes of testing, the gas source should be turned off to cool the instrument for 15 minutes.

6. Ambient airflow: No forced air movement phenomena during operation;

7. The instrument should be placed in a fume hood for testing.

Divided into two main parts: 

1, the smoke chamber;

2, the control section;


Smoke chamber section: On the left and right side panels of the smoke chamber, there are the power switch, safety symbol switch (backlight switch), gas adjustment device, and also the switch for controlling the exhaust fan (fan switch).


ASTM D2843-22 

Standard Test Method for Density of Smoke from the Burning or Decomposition of Plastics


Main Technical Specification

Maximum smoke density (MSD) , 

smoke density grade (SDR) of the test specimen

Continuous measurement from 0-100%, automatically calculated
Calibration error with standard filter platesno more than 3%
Working   pressure of the Bunsen burner(210±5) KPa
Time of Bunsen burner applies flame to the sample4 minutes
Combustion lampBunsen burner, with a length of 260mm and a nozzle diameter of 0.13mm, forming a 45° angle with the smoke box
Photoelectric systemLight source is a bulb, with a power of 15W and a working voltage of 6V
Exhaust systemequipped with a powerful exhaust fan, capable of expelling waste gas outdoors after testing
Smoke density measurement range0~100%
Smoke density measurement accuracy±3%
Receivera silicon photodiode, 0% transmittance indicates no light passes, 100% transmittance indicates unobstructed light passage
Main burner working pressure276KPa (adjustable), auxiliary burner optional
Touch display screen

a. Size: 5 inches effective display size, length 11cm, width 6.28cm; 

b. Resolution: 800*480 

c. Communication interface RS232, 3.3V CMOS or TTL, serial mode 

d. Storage capacity: 1G 

e. Uses pure hardware FPGA to drive the display, "zero"   startup time, runs upon powering on 

f. Uses M3 FPGA architecture, M3 is responsible for instruction parsing for FPGA TFT display, with good speed and reliability 

g. The main controller uses low-power processors, automatically   enters energy-saving mode

Gas source95% propane gas or gas of equivalent purity (provided by customer)
DimensionsLength*Width*Height: 740*500*900 (mm)

Automatic timing, automatic ignition, automatic smoke exhaust;   

luminous flux can be linearly corrected in stages for accurate test data