Home >> Products >> Industrial Specialized Testing >> Civil Engineering >> Intelligent universal Sand Strength Machine
Intelligent universal Sand Strength Machine

Intelligent universal Sand Strength Machine

Model: UT4151

Intelligent universal Sand Strength Machine used to measure the compression, shear, flexural, tensile strength of mold(core) sand. Using automatic mechanical loading, sensor data collection, digital table directly display test results, and can maintain the maximum destructive value.  With data storage, output printing function. With computer interface (including software), equipped with 485-232 conversion interface, data processing generated.txt file (txt format file). 


Intelligent universal Sand Strength Machine, molding sand strength test. 


General Introduction

Intelligent universal Sand Strength Machine used to measure the compression, shear, flexural, tensile strength of mold(core) sand. Using automatic mechanical loading, sensor data collection, digital table directly display test results, and can maintain the maximum destructive value.  With data storage, output printing function. With computer interface (including software), equipped with 485-232 conversion interface, data processing generated.txt file (txt format file). 


Intelligent universal Sand Strength Machine, molding sand strength test. 

Main features

  • Key feature

Using automatic mechanical loading, sensor data collection, digital table directly display test results

Maintain the maximum destructive value. 

With data storage, output printing function. 

With computer interface (including software), equipped with 485-232 conversion interface, data processing generated.txt file (txt format file). 

Main Technical Specification

Max. push force10000N (10KN)
Measurement   range0—10000N
Measurement range for sand mold testingCompressive strength: 0-5Mpa
Tensile strength: 0-18MPa
Shear strength: 0-1.2MPa
Bending strength: 0-60MPa
Measurement accuracy±1.5%
PowerAC   220V, 50HZ, 1 phase


Main accessories

Frame   1 set

Test fixture 1 set (for compressive, shear, bending, and tensile strength)

Power cord 1 pc

Brush   1 pc

Micro-printer   1 set

Manual etc., 1 set