Information on the most widely used ASTM standards within the materials testing industry
Model: UT4066
UT4066 Sodium bentonite geosynthetic clay liner hydrostatic pressure testing machine, or name Sodium-based bentonite waterproof blanket hydrostatic water Pressure Tester used to determine the resistance to static water pressure of sodium-based bentonite waterproof blankets.
General Introduction
UT4066 Sodium bentonite geosynthetic clay liner hydrostatic pressure testing machine, or name Sodium-based bentonite waterproof blanket hydrostatic water Pressure Tester used to determine the resistance to static water pressure of sodium-based bentonite waterproof blankets.
Main features
When the pressure difference on both sides of the sodium-based bentonite waterproof blanket reaches a certain value, the waterproof blanket will be destroyed. Gradually increase the hydraulic pressure difference on both sides of the sample and maintain it for a certain period of time. When water begins to flow out of the outlet, it indicates that the sample has been destroyed, thus obtaining the sample's resistance to static water pressure.

1. All stainless steel surface, acid-resistant, alkali-resistant, corrosion-resistant, easy to clean.
2. Touch display screen, automatic pressurization.
0.4Mpa or 0.6Mpa in one hour hydrostatic pressure test, without leakage.

Main Technical Specification
1. Sample diameter: φ55mm
2. Maximum test force: 2.0MPa
3. Pressurization rate: 0.1MPa/h can be set
4. Number of samples that can be processed at one time: 3 pieces
5. Dimensions: 610x730x1850 (mm)
6. Weight: 80Kg
Require More Customized Solutions?