Model: UT4014
UT4014 Concrete Water Permeability Testing Machine is suitable for concrete impermeability test and determination of anti-seepage level, it can also be used to determine the permeability of building materials and quality inspection. As a result, it has been widely used in the production, construction, design, scientific research and other departments.
Mainly the pressure value through the sensor on the pressure display, and according to the set of procedures to achieve automatic rising pressure, automatic completion of the test.
General Introduction
UT4014 Concrete Water Permeability Testing Machine is suitable for concrete impermeability test and determination of anti-seepage level, it can also be used to determine the permeability of building materials and quality inspection. As a result, it has been widely used in the production, construction, design, scientific research and other departments.
Mainly the pressure value through the sensor on the pressure display, and according to the set of procedures to achieve automatic rising pressure, automatic completion of the test.
Main Technical Specification
| Max. working pressure | 4.0Mpa |
| Working mode | Automatic constant pressure |
| Specimens number | 6 pcs |
| Specimen mold dimension | Upper open diameter: 175m mLower open diameter: 185mm Height: 150mm(Mold size customized) |
| Plunger pump parameter | Diameter: 10mm, stroke: 10mm Frequency: 154 times/min. Flow rate: 0.11L/min |
| Motor power | 220V, 50HZ, single phase, 90W |
| Dimensions | 960*650*980mm |
| Weight | 200Kg |
Main Accessories
1, Frame
2, Test mould (6 pcs)