Information on the most widely used ASTM standards within the materials testing industry
Model: UT1016B
ASTM F1160 Rotary Bar Bending Strength Fatigue Test Machine or name Rotating Beam Tester, a sample is placed in the machine and a force is applied via a bending moment from a secondary actuator. The force induces a surface stress that will be tensile on one side of the sample and compressive on the opposite side. When the test is started, the sample will rotate at the desired rate and this rotation will cause the surfaces to interchange so that each surface experiences alternating tensile and compressive stresses. The sample is left in the machine until failure at which point will display the number of cycles it took for the sample to fail. Running a series of tests on identical samples with varying stresses will allow the user to create an S-N curve.
UnitedTest Rotary Bar Bending Strength Fatigue Test Machine is used for conducting small sample cantilever pure bending fatigue tests on black metal and its alloy materials under room temperature and high temperature conditions, to determine the fatigue performance of metal circular cross-section test samples under bending moment under rotating state.
General Introduction
ASTM F1160 Rotary Bar Bending Strength Fatigue Test Machine or name Rotating Beam Tester, a sample is placed in the machine and a force is applied via a bending moment from a secondary actuator. The force induces a surface stress that will be tensile on one side of the sample and compressive on the opposite side. When the test is started, the sample will rotate at the desired rate and this rotation will cause the surfaces to interchange so that each surface experiences alternating tensile and compressive stresses. The sample is left in the machine until failure at which point will display the number of cycles it took for the sample to fail. Running a series of tests on identical samples with varying stresses will allow the user to create an S-N curve.
UnitedTest Rotary Bar Bending Strength Fatigue Test Machine is used for conducting small sample cantilever pure bending fatigue tests on black metal and its alloy materials under room temperature and high temperature conditions, to determine the fatigue performance of metal circular cross-section test samples under bending moment under rotating state.
This testing machine adopts a cantilever beam structure, consisting of a frame, an AC high-speed motor and driver, a measurement and control system, a loading weight, a high-temperature furnace and controller, a high-temperature fixture, a lubrication device, a protection device, etc. The equipment has a rotation counter.

The fixture uses elastic front and rear clamps to hold the sample, and the clamp is connected to the spindle elastic cylinder clamp to achieve precise fit, ensuring that the radial runout of the clamped sample meets the requirements of navigation marks and national standards.

Key Features
1, Equipped with touch screen operation and display panel for the completion of all control parameters of the setting, all measurement data display and all test operations, equipped with a network interface with computer communication, elected with the computer, can realize the computer to a single device measurement and control or the network of multiple devices, test weekcan can be set at will, to reach the set value can be automatically stopped and has power-down protection function.
2, Both front and rear fixtures are clamped in an elastic cone sleeve for a sample, enabling precision fit.
3, ple break automatic shutdown protection, etc., equipment equipped with transparent housing, the test process can be unattended.
4, When the computer is configured, a single test machine or multiple test machines can be centralized and controlled. The computer takes WIN10 as the working platform, adopts the virtual panel operation mode, the interface is clear, the operation is convenient, the program specification is stable, completes the management control of the whole equipment, the test data collection and processing and storage and printing; Its format can also be converted to commonly used software document formats such as Word, Excel, and so on.
DIN 50113:2018-12 Testing of metallic materials - Rotating bar bending fatigue test
ISO 1143-2010: Metallic materials - Rotating bar bending fatigue testing
ASTM F1160-14(2017)e1 Standard Test Method for Shear and Bending Fatigue Testing of Calcium Phosphate and Metallic Medical and Composite Calcium Phosphate/Metallic Coatings
BS EN 13261:2024 Railway applications. Wheelsets and bogies. Axles. Product requirements
Main Technical Specification
| Max. rotate speed (selection) | 1-1500rpm 1-3000rpm 500-6000rpm 500-12000rpm |
| Max. loading force | 2000N.CM |
| Loading arm of force | 100mm; relative error: ≤±0.3%; adjustable spacing between left and right clamps |
| Right and right fixture coaxial | ≤Փ0.02mm |
| Static radial run-out | ≤0.02mm |
| dynamic radial run-out | ≤0.06mm |
| Specimen length | 226 mm |
| Temperature in spindle box | ≤ 30℃ |
| Bend moment relative error | ≤±1% |
| Counter | 108 |
| Power supply | 380V, 50HZ, 3 phase, 1Kw |
Optional Mandrel
| Frame structure | 1 set |
| Measuring and control system | 1 set |
| Loading system and weights | 1 set |
| Speed adjusting system | 1 set |
| Computer | 1 set |
| English software | 1 set |
| Clamping grips | 1 set |
| Documents (Manual, packing list, certificate) | |