Tensile Testing || Strip test || Grab Test || Tearing test of Fabric
Date:2022-05-18 Source:United Test Views:100

Fabric Tensile Strength Test | Strip Strength Test | Grab strength test | Tearing strength test | Elmendorf Tear Test | Bursting strength  ASTM D5035, ISO 13934-1

The strip test is a tensile test in which the full width of the test specimen is gripped in the tensile grip jaws of a universal testing machine. During this test, tensile force is applied on the fabric specimen until it ruptures. Mechanical properties to analyze include the force at rupture and the elongation (expressed as percentage) at maximum force and/or at rupture.