Your current locationHome>Application>Test Type>other special test
Application
other special test
Molding sand strength test (tensile, shear, compression test).
Date:2025-06-20 Source:United Test Views:100

The mold sand strength test is a series of tests used to measure the resistance to failure of mold sand under external forces. 

Mold sand strength refers to the ability of mold sand to resist failure when subjected to external forces, including compression, shear, tensile, and bending strength.Testing MethodsThe specific methods for mold sand strength testing include the following:

- Compressive Strength: Place a standard cylindrical sample between pressure plates and apply vertical pressure until rupture, recording the maximum load at failure and calculating the stress per unit area.

- Shear Strength: Apply shear force to the sample and measure the load at transverse fracture.

- Tensile Strength: Use a figure-8 shaped sample or bonded sample, applying tensile force until rupture.


Testing Equipment

The equipment for conducting mold sand strength tests mainly includes:

- Unitedtest UT4151 Universal Strength Testing Machine: Equipped with different fixtures to apply various external forces.- Mold Sand Strength Testing Instrument: Specifically designed for testing the strength of mold sand.


Testing Steps- Sample Preparation: Prepare the sample according to standards, uniformly mix mold sand and fill it into a standard sample cylinder, compacting it using a hammer-type sample preparation machine. Wet samples are tested directly, while dry samples need to be dried and cooled to room temperature.- 


Equipment Calibration: Check the zero point of the instrument and ensure the loading speed meets standards (e.g., 1-2 mm/min).- 

Testing Process: Place the sample on the testing platform, adjust the fixture position, start the equipment, and uniformly load until the sample ruptures, recording the maximum load value.- 

Calculation: Strength = Maximum Load / Sample Cross-Sectional Area (adjusted based on sample dimensions).

Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X