ISO 974 Plastics — Determination of the brittleness temperature by impact
Date:2024-12-06 Source:United Test Views:100

Scope:

Brittleness temperature is the temperature at which 50% of the tested specimens exhibit brittle failure at specified impact conditions. It is utilized primarily for plastics and elastomers.


Test Procedure:

Specimens are secured in the customer specified specimen holder (A or B) with a torque wrench at 5 in-lb. The specimen holder is lowered into a bath at a specified temperature. The specimens are impacted at 2000 ± 200 mm/s and then examined. The procedure is repeated at a lower temperature until enough data is generated to determine a brittleness temperature. Brittle temperature is the temperature at which 50% of the specimens fail. Brittle failure is defined by ASTM D746 as fracture into 2 or more pieces, or any crack visible to the unaided eye. The specimens can be bent to an angle of 90° and examined for cracks at the bend.


Data:

Test temperatures, number of failures and the determined brittleness temperature.


Specimen size:

There are three specimens: Type I, Type II or Type III. ASTM specimens are Type I at 6.35 mm by 31.75 mm by 1.91 mm thick. ISO specimens are Type III at 20 mm by 2.5 mm and 2.0 mm thick.


Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X