ISO 4422-2 Pipes and fittings made of unplasticized poly (vinyl chloride) (PVC-U) for water supply - Specifications - Part 2: Pipes (with or without integral sockets).
Date:2022-11-02 Source:United Test Views:100

ISO 4422-2:1996Pipes and fittings made of unplasticized poly (vinyl chloride) (PVC-U) for water supply - Specifications - Part 2: Pipes (with or without integral sockets). It specifies the characteristics and properties of extruded pipes made of unplasticized poly (vinyl chloride) (PVC-U), with or without socket(s) (integral or not), intended to be used for buried water mains and services and for water suppliers above ground, both inside and outside buildings.