ISO 182-1 PVC compounds thermal stability test Congo red method
Date:2025-05-29 Source:United Test Views:100

ISO 182-1 PVC compounds  thermal stability test Congo red method. The determination is carried out on a sample of the PVC compound which is maintained at an agreed temperature in still air until the colour of a Congo red paper held above it changes from red to blue. If universal indicator paper is used, the colour change is that corresponding to pH 3.

 微信图片_20250529191614.png

This test method is intended to determine the thermal stability of a PVC compound when processed at a high temperature. The method is applicable to all PVC compounds, copolymers and products based on them. A test specimen of the PVC material is heated at a defined temperature, normally 180°C.


Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X