GOST 30599 Wheels made of lightweight alloys for pneumatic tires. Technical requirements and testing methods.
Date:2025-04-12 Source:United Test Views:100

GOST 30599 Wheels made of lightweight alloys for pneumatic tires.-Specification for road wheels manufactured wholly or partly of light alloy for mopeds and motor cycles; specifies test methods for evaluating the performance of passenger car wheels intended for use on roads. The standard outlines a series of tests that assess the strength, durability, and performance characteristics of these wheels, with the goal of ensuring they meet the necessary safety and quality requirements for use on the road.

The tests outlined in GOST 30599  include radial fatigue testing, cornering fatigue testing, impact testing, and more. These tests simulate real-world driving conditions and help to ensure that the wheels can withstand the stresses and strains of regular use over time. So, By adhering to the standards outlined in the standard, manufacturers can ensure that their passenger car wheels are safe and reliable for use on the road.

Requirements of GOST 30599 

Radial fatigue testing: This test is used to evaluate the resistance of the wheel to repeated bending loads applied in a radial direction. The test measures the number of cycles the wheel can withstand before failure occurs.

439761b4ff26600f6dc311cf166e1d70.png

Cornering fatigue testing: This test evaluates the ability of the wheel to withstand repeated bending loads applied in a lateral direction. The test measures the number of cycles the wheel can withstand before failure occurs.

Impact testing: This test evaluates the ability of the wheel to withstand an impact from a curb or other obstacle. The test measures the force required to cause visible damage to the wheel.

13c3655aa8413e052a1640905bad3a3e.png

Coating adhesion testing: This test evaluates the adhesion of the coating to the wheel. The test measures the force required to peel off the coating from the wheel surface.

Dynamic cornering fatigue testing: This test evaluates the ability of the wheel to withstand repeated bending loads applied in a lateral direction while the wheel is rotating at high speeds. The test measures the number of cycles the wheel can withstand before failure occurs.

333b12a30229a3a63c82e422fd173c47.png

Dynamic radial fatigue testing: This test evaluates the ability of the wheel to withstand repeated bending loads applied in a radial direction while the wheel is rotating at high speeds. The test measures the number of cycles the wheel can withstand before failure occurs.

image.png

GOST 30599 Wheels made of lightweight alloys for pneumatic tires. Technical requirements and testing methods. Testing Machine

Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X