ASTM D2992 Fiberglass Glass-Fiber-Reinforced Thermosetting-Resin Hydrostatic Pressure Test
Date:2025-04-14 Source:United Test Views:100

ASTM D2992 Fiberglass Glass-Fiber-Reinforced Thermosetting-Resin Hydrostatic Pressure Test

This practice is useful for establishing the hoop stress or internal pressure versus time-to-failure relationships, under selected internal and external environments which simulate actual anticipated product end-use conditions, from which a design basis for specific piping products and materials can be obtained. This practice defines an HDB for material in straight, hollow cylindrical shapes where hoop stress can be easily calculated, and a PDB for fittings and joints where stresses are more complex.  

This practice establishes two procedures, Procedure A (cyclic) and Procedure B (static), for obtaining a hydrostatic design basis (HDB) or a pressure design basis (PDB) for fiberglass piping products, by evaluating strength-regression data derived from testing pipe or fittings, or both, of the same materials and construction, either separately or in assemblies. Both glass-fiber-reinforced thermosetting-resin pipe (RTRP) and glass-fiber-reinforced polymer mortar pipe (RPMP) are fiberglass pipe.

ASTM D2992 Hydrostatic Pressure Testing Machine for Fiberglass Glass-Fiber-Reinforced Thermosetting-Resin Hydrostatic Pressure Test pipe sample:

pipe hydrostatic pressure testing machine, ISO 1167.jpg

Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X