ASTM C1674 Flexural Strength Test of Advanced Ceramics with Engineered Porosity
ASTM C1674 is an international ASTM test method for measuring the flexural strength of advanced ceramics with engineered porosity at ambient temperatures.
ASTM C1674 test method is used to determine the mechanical properties in flexure of engineered ceramic components with multiple longitudinal hollow channels, commonly described as “honeycomb” channel architectures. The components generally have 30 % or more porosity and the cross-sectional dimensions of the honeycomb channels are on the order of 1 mm or greater.