ISO 13007-4 flexural and compression test of Ceramic tiles — Grouts and adhesives
Date:2025-07-26 Source:United Test Views:100

ISO 13007-4 flexural and compression test of Ceramic tiles — Grouts and adhesives


ISO 13007-4 Ceramic tiles — Grouts and adhesives Part 4: Test methods for grouts

ISO 13007-4  standard describe the methods for determining characteristics for grouts used in internal and external installation of ceramic tiles.


Test methods: 

-   Determination of flexural and compressive strength;

-   Determination of water absorption;

-   Determination of shrinkage;

-   Determination of resistance to abrasion);

-   Determination of chemical resistance.

e2102483c9f833ae5339b89e96b840de.png

Flexural test

0ca969db66f1caf79fcdf93838fff49e.png

Compression test

Related products
Contact

Email:
export@unitedtest.com
unitedtest@hotmail.com
Tel:
+86-10-57055071
+86-13911165373

MS Teams: 
unitedtest@hotmail.com

WhatsApp:
+86 13911165373

WeChat:
UnitedTest-V1 

X