Home >> Products >> Industrial Specialized Testing >> Abrasion & Wear Test >> Coating Scratch resistance tester
Coating Scratch resistance tester

Coating Scratch resistance tester

Model: UT2091A. ASTM C217, BS EN 13310

UT2091A Scratch Resistance Tester is used to evaluate the shear, scratch, planing, scratching and engraving properties of materials. The equipment is simple to operate and easy to move.


Ability to test samples of squares or rounds 1/2" to 4" thick. By changing the position of the sliding weight, the load on the sample can be adjusted in the range of 0-1000g. Cutting tools can be made with either tungsten carbide tools or conical diamond heads. The reproducibility of experimental data can help manufacturers effectively control production and test the performance of products.


1.1 Before the instrument is tested, the scale rod needs to be adjusted to the appropriate height according to the thickness of the sample. Attach the tight cutting tool to the scale bar and place it on the sample. Start the instrument, and the constant speed of the turntable ensures that the test results are accurate. By varying the load of the cutting tool, it is possible to evaluate the scratch resistance of the material.

1.2. The design of the scale bar of the instrument makes it possible to be at the level of the sample and the turntable, and can be raised or lowered according to the actual needs, in addition, the scale bar can also be lifted and suspended in the air to facilitate the operator to remove the sample.

General Introduction

UT2091A Scratch Resistance Tester is used to evaluate the shear, scratch, planing, scratching and engraving properties of materials. The equipment is simple to operate and easy to move.


Ability to test samples of squares or rounds 1/2" to 4" thick. By changing the position of the sliding weight, the load on the sample can be adjusted in the range of 0-1000g. Cutting tools can be made with either tungsten carbide tools or conical diamond heads. The reproducibility of experimental data can help manufacturers effectively control production and test the performance of products.


1.1 Before the instrument is tested, the scale rod needs to be adjusted to the appropriate height according to the thickness of the sample. Attach the tight cutting tool to the scale bar and place it on the sample. Start the instrument, and the constant speed of the turntable ensures that the test results are accurate. By varying the load of the cutting tool, it is possible to evaluate the scratch resistance of the material.

1.2. The design of the scale bar of the instrument makes it possible to be at the level of the sample and the turntable, and can be raised or lowered according to the actual needs, in addition, the scale bar can also be lifted and suspended in the air to facilitate the operator to remove the sample.

Main features

  • Application
  • Standard

The instrument is used to test rigid organic materials, coating adhesives, powder coating anodizing materials, soft metals, plastics and glass, etc., and can also be used for the adhesive quality of protective coatings of the same material and the ultimate performance test of similar materials, which is widely used in product quality control, new product development performance verification, testing agency testing and other fields.

AS/NZS AS2924.2, 

ASTM C217,  

BS EN 438.2,

BS EN 13310, 

BS EN 14323,  

BS EN 14688,    

DIN 53799, 

DIN 68861-4

Main Technical Specification

Control ScreenIntelligent Electronic   Counter/Timer
Test ModeAutomatic
Test speed1RPM/5RFM
Travel range360 degrees
Test area1/2" to 4"
Scraping head sizearbitrarily   interchangeable
Applied load5N/10N range stepless   adjustment
Test sample thickness20mm
WEIGHT25kg
Power220V,   50HZ, 45W
Dimension750*330*390mm


Main Accessories

5N weights (adjustable) ;  

Balance weights;    

Scraping Head Kit (ASTM) ;   

Scraping head (diameter 0.09)

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.