Plastic Film and sheets tensile test ISO 527-3 is a common international standard that is used to determine the tensile properties of plastic film or sheeting - a plastic test specimen with a thickness less than 1 mm. The tensile properties include tensile strength, yield strength, yield strain, strain at break, and in some cases Young's Modulus. Due to the flexible, delicate nature of these plastic specimens, both gripping and strain measurement can be a challenge.

Refer UnitedTest single column electronic universal testing machine, load range 100N ~ 5Kn.   because thin test sample, recommend the pneumatic side-action grips.

Plastic Film and sheets tensile test ISO 527-3

ISO 527-3 Tensile Test of Plastic Thin Film Sheet

ISO 527-3 covers the specimen preparation requirements of thin plastic sheets and films. Thin plastic specimens created with the practices of ISO 527-3 are tensile tested with the practices of ISO 527-1. Thin plastic specimens created in accordance with ISO 527-3 are cut, or punched from a sheet of thin plastic.

ISO 527-3 specifies that thin plastic film of sheet specimens must be free from cracks or scratches that will affect the tensile test. ISO 527-3 allows for four specimen geometries that can be used for tensile testing. There are three acceptable dogbone shaped specimens that are acceptable. Specimen created following ISO 527-3 can be used to determine the tensile properties of thin plastic sheets and films including the tensile modulus of elasticity and the tensile energy to break (TEB).

< Previous: Pipe fittings pull out resistance testing machine, Tensile Pull Out Test

> Next: Tensile Test of Moulding and Extrusion Plastics ISO 527-2

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.