UT4016 hydraulic type Automatic Fabric Bursting Strength Tester is used test burst strength in a variety of textiles, nonwovens, paper, cardboard, plastics and medical products.
Conform to standard: ISO 13938.1, Textiles — Bursting properties of fabrics — Part 1: Hydraulic method for determination of bursting strength and bursting distension.
FZ/T 60019、FZ/T 01030、ASTM D3786、BS 4768、WOOLMARK TM 29、WSP 30.1、JIS L 1018.6.17; GB/T 7742.1-2005
Working mode | Touching screen, data printing |
Measuring range | 2.0Mpa |
Resolution | 0.001KPa |
Elastic diaphragm thickness | ≤2mm |
Measuring accuracy | 0.2%FS |
Sample size | Standard with delivery is 50cm²
Optional: 7.3 cm²(Φ30.5mm), 10 cm²(Φ35.7mm), 50 cm²(Φ79.8mm), 100 cm²(Φ112.8mm) |
Maximum expansion | 75mm |
Pressure rising rate | 20-600ml/min |
Measuring unit | kpa,kgf/ cm2,lb/in2 free change |
Test methods | constant speed expansion, constant pressure, fixed dilation and timing |
Power | AC 220V, 50HZ. 100w |
Weight | 125kg |
Dimensions | 530*620*840mm |
Tools,
Diaphragm
ISO 13938.1, Textiles — Bursting properties of fabrics — Part 1: Hydraulic method for determination of bursting strength and bursting distension.