ISO 62 Water Content Analyzer, Moisture Tester, Moisture absorption properties
UnitedTest Halogen Moisture Analyzer works for the injection of iodine or bromine and other halogen gas in the bulb, at high temperature, the sublimation of tungsten and halogen chemical action, sublimation of tungsten on tungsten will re-solidify to form a balanced cycle, to avoid premature rupture of tungsten. Therefore live longer than incandescent halogen bulbs. And because the filament can work at higher temperatures, resulting in a higher brightness, higher color temperature and higher luminous efficiency.
Moisture Analyzer distinguish it from other products in that moisture traditional oven drying method is generally used to test a sample of three or even take two or three or four hours and needs by weighing scales, manual calculation, in order to obtain Moisture value (water content) of the sample. Low efficiency of traditional oven method of moisture determination, not able to adapt to the fast pace of production needs. It’s high efficiency of the drying heater - high quality ring halogen, samples are quick and uniform heating, water samples continued to be dried. The entire measurement process, rapid moisture analyzer fully automated real-time display of measurement results: Sample weight, moisture content, solids, measurement time, the heating temperature. Cheap Halogen Moisture Analyzer application of the international principle oven drying, moisture determination with the oven method of measurement of a good consistency, efficiency is much higher than the moisture determination oven method. Use Halogen Moisture Analyzer, general sample measurement is completed only a few minutes, so by the business users love and praise. Conform with ISO 62 standard.
ISO 62:2008 Plastics — Determination of water absorption
ASTM D570-22 Standard Test Method for Water Absorption of Plastics
Features:
2.1. No need to install & commissioning
2.2. Easy Operation and no need use training
2.3. Short test time and high efficiency
2.4. Heating uniformity, stable performance, high accuracy
2.5. Small size and light weight
2.6. Automatic measurement, End buzzer, Without care when working
2.7. Versatile, suitable for almost all sectors of moisture determination
2.8. High performance electromagnetic force sensor, the maximal capacity can reach 1mg readability, provide the best measured performance.
2.9. Unique windscreen design, makes the weighing system more stable
2.10. Pure stainless steel heating chamber cavity cover, high temperature, easy to clean.

Max. Weight | 50g |
Weighing Readability | 1mg (0.001g) |
Repeatability(Standard Error) | ±0.01% |
Operational Temperature Range | 13-25℃ Best |
Suggest Sample Weight(g) | 3 - 10 g |
Pan (mm) | 100mm |
Heat Time | 1 - 99 minutes (stepping is 10 seconds.) |
Display Screen | LCD (Liquid Crystal Display) |
Heating method | Halogen |
Interface | RS232 |
Power | 220V, 50HZ |
Heating Temperature Range | 50-180℃ |
Display | Solid %, Moisture %, Weight, Time, Temperature |
Dimensions | 285×160×150mm |
Weight | N.W.: 3.3kg, G.W: 5kg |
ISO 62:2008 Plastics — Determination of water absorption
ASTM D570-22 Standard Test Method for Water Absorption of Plastics