- Universal testing machine
- Fixtures
- Medical/Biomedical device
- Vehicles motorcycle
- Compression/Flexural test
- Hardness tester
- Impact testing machine
- Torsion testing machine
- Abrasion & wear tester
- Plastic & Pipe testing
- Tensiometer / Goniometer
- Erichsen cupping tester
- Other Testing Equipment
- Grinding & polishing machine
- Spring testing machine
- Introduction
- Specification
- Accessories
- Standard
- LEAFLET & VIDEO
- Contact Us
RST series ring stiffness tester is used to determine the ring stiffness of circular cross-section thermoplastic pipes, according customer’s request, it can also execute compression, ring stiffness, ring softness and creep ratio test. This tester meet the requirement of all kinds of plastic pipes, structured-wall pipes, PVC, HDPE, LDPE, PE corrugated pipes, helically wound pipes etc.,
Conform with Standard ISO 9969, ISO 9967. ASTM D2412, EN1446, ISO 9969 Plastic pipe ring stiffness test, AS 1462.22
Feature of RST-2 series:
Suitable for small or middle size pipe test (1000mm dia.); computer control, High level quality.
Principle of ring stiffness:
The ring stiffness is determined by measuring the force and the deflection while deflecting the pipe at a constant deflection speed.
A cut length of pipe supported horizontally is compressed vertically between two parallel flat platens moved at a constant speed that is dependent upon the diameter of the pipe.
A plot of force versus deflection is generated. The ring stiffness is calculated as a function of the force necessary to produce a 3% diametric deflection of pipe.
Principle of creep ratio:
A cut length of pipe is placed between two parallel flat horizontal plates and a constant compressive force is applied for 1008 h (42 days). The deflection of the pipe is recorded at specified intervals so as to prepare a plot of pipe deflection against time. The linearity of the data is analysed and the creep ratio is calculated as the ratio between the two years’ extrapolated deflection value and the measured 6 min (0.1 h) deflection.
Other name:
Pipe ring stiffness tester, PVC pipe ring stiffness test, HDPE pipe ring stiffness testing equipment, PE pipe creep rate test, thermoplastic pipe creep ratio test. RST-2 pipe ring stiffness testing machine ISO 9969
Test procedure:
1. The test should be conducted under conditions of 23°C ± 2°C.
2. If it can be determined that the ring stiffness at a certain position of the sample is minimal, make contact between the sample 'a' at that position and the platen of the press, or when placing the first sample, place the other two samples 'b' and 'c' at positions relative to the first sample, rotating them by 120° and 240° respectively.
3. For each sample, properly place the deformation measuring device and check the angular position of the sample. When placing the sample, keep its long axis parallel to the platen, and then position it at the center of the testing machine. Ensure that the upper platen just contacts the sample and can hold it, compressing the sample at a constant speed until a deformation of at least 0.03d is reached.
4. Typically, the amount of deformation is obtained by measuring the position of a platen, but if during the sample process, the change in wall thickness 'e' exceeds 10%, then the change in the inner diameter of the sample should be obtained through the measurement of the diameter.
| Model: RST-1 series | Suitable for small size pipe test (less 630mm dia.); |
| Model: RST-2 series | Suitable for small or middle size pipe test (less than 1000mm dia.) |
| Model: RST-3 series | Suitable for large size pipe test (over 1000mm dia.) |
| Max. load | 10KN, 20Kn, 30Kn, 50Kn, 100Kn |
| Load resolution | 0.01N |
| Load cell quantity | 1 to 3 pcs |
| Load accuracy | ±1% of reading value |
| Crosshead travel | 100mm-3500mm |
| Pipe Diameter range | 16mm to 3200mm |
| Speed range of crossbeam | 0.1 mm/min~500 mm/min, stepless, adjustable freely |
| Width of test space | 420mm to 1000mm |
| Displacement accuracy | 0.001mm |
| Power | 220V/380V, 50Hz/60HZ |
| Pipe inner diameter measuring device | YES |
| Creep Ratio Test(option) | ISO 9967 |
| Time range | 1~9999h59min59s |
| Timing resolution | 1s |
| Item | Quantity |
| Frame | 1 set |
| (include load cell, servo motor etc.,) | |
| Compression platen (400*400mm) | 1 set |
| Pipe inner diameter measuring device | 1 set |
| Computer (English Win7) | 1 set |
| Professional ring stiffness test software (English) | 1 set |
| Documents (Manual, packing list, certificate) | |
ISO 9969 "Thermoplastics pipes -- Determination of ring stiffness”
ISO9967 "Thermoplastics pipes -- Determination of creep ratio“
ASTM D2412, EN1446, AS 1462.22