Metallographic equipment consumables
- Introduction
- Specification
- Accessories
- Standard
- LEAFLET & VIDEO
- Contact Us
Supply wide range consumable material for grinding, polishing and mounting press.
Diamond Disc, Diamond cutting disk, Metallographic sand paper, Abrasive pastes, polishing powder, polishing agent, Mounting press consumable
| Name | Description | Specification | Package |
| Diamond cutting disk | Saw is made by edge electroplate technology, widely used for ceramic, glass, alloy etc., thin piece precision cutting. | Φ100×0.4×12.7mm | In bulk |
| Φ150×0.4×12.7mm | In bulk | ||
| Saw is made by edge sintered technology, with high precision, long life character. Used for hard alloy, brittle metal etc. precision cutting. | Φ100×0.5×12.7mm | In bulk | |
| Φ125×0.5×25.4mm | In bulk | ||
| Φ150×0.6×25.4mm | In bulk | ||
| Φ200×1×25.4mm | In bulk | ||
| Φ200×1×32mm | In bulk | ||
| Cooling lubricating liquid. | With high cooling, lubricating, anti-rust ability. | 1:20concentrated liquid, use water to dilute. | 1000ml/bottle |
Sand paper:
| Name | Description | Granularity | Specification | Package |
| Waterproof sand paper | Black silicon carbide, uniform and durable | 240#,400#,600#,800#, 1000#,1200#1500#,2000# | Φ200mm with gum | 50pc/case |
| 240#,400#,600#,800#,1000# | Φ250mm no gum | 100pc/case | ||
| 240#,400#,600#,800#,1000# | Φ300mm no gum | 100pc/case | ||
| Metallographic sand paper | Green silicon carbide, uniform, dry and wet. | 120#~4000# | Φ200mm with gum | 50pc/case |
| Φ200mm no gum | 50pc/case |
Polishing Wave:
| Material | With gum | No gum | package |
| Velvet | Φ200mm | Φ250mm | 15pcs/case |
| Panne velvet | Φ200mm | Φ250mm | 15pcs/case |
| Worsted | Φ200mm | Φ250mm | 15pcs/case |
| Canvas | Φ200mm | Φ250mm | 15pcs/case |
| Wool felt | Φ200mm | Φ250mm | 15pcs/case |
| Velvet | Φ250mm | Φ300mm | 15pcs/case |
| Panne velvet | Φ250mm | Φ300mm | 15pcs/case |
| Worsted | Φ250mm | Φ300mm | 15pcs/case |
| Canvas | Φ250mm | Φ300mm | 15pcs/case |
| Wool felt | Φ250mm | Φ300mm | 15pcs/case |
Mounting press consumables:
| Urea-formaldehyde molding powder | White, for general sample preparation. | 4kg/barel |
| Bakelite owder | Black, for general sample preparation. | 4kg/barel |
| Hot mounting press inlay | Red, for electric conduction sample, like electron microscope, electrochemical polishing. | 500g/bottle |
| Hot mounting press inlay | Green, for high requirement for sample edge | 500g/bottle |
| Cold mounting press inlay | Semitransparent, for can not heating sample or no mounting press equipment place | 500g/bottle (cold mounting powder); 500ml/bottle (cold mounting liquid); Φ30mm(1 pc cold mounting mold) |
| Crystal inlay | Transparent, for can not heating sample or no mounting press equipment place | 1000ml/bottle(cold mounting liquid),50ml/bottle(Curing agent);Φ30mm(1 pc cold mounting mold) |
| Cold mounting press mold | Can repeatable use | Φ20mm,Φ40mm,Φ50mm,40×25mm |
| Cold mounting press mold | Can repeatable use | Φ25mm,Φ30mm |
| Mounting press sample holder | Plastic | 500pc/bag |
| Release agent | For hot mounting press and cold mounting mold demould. | 350ml/bottle |