- Universal testing machine
- Fixtures
- Medical/Biomedical device
- Vehicles motorcycle
- Compression/Flexural test
- Hardness tester
- Impact testing machine
- Torsion testing machine
- Abrasion & wear tester
- Plastic & Pipe testing
- Tensiometer / Goniometer
- Erichsen cupping tester
- Other Testing Equipment
- Grinding & polishing machine
- Spring testing machine
- Introduction
- Specification
- Accessories
- Standard
- LEAFLET & VIDEO
- Contact Us
The ASTM F543 standard specifies the torque required to measure the insertion and extraction of metal bone screws from standard materials, in order to confirm the consistency of the tested product. Load maintains 11.17N and rotates at a rate of 3r/min for 4 turns, followed by 4 turns.
The UnitdTest UT1050 series Metal bone screw torsion testing equipment has a lightweight body, easy operation, and precise control, making it suitable for bone nail testing. We provide you with professional testing fixtures to meet standard requirements, as well as precise and effective test plans (SOP), and optional data post-processing software to reduce the difficulty of data processing and assist in the mechanical performance analysis of metal bone screws.
Product features:
A new generation fatigue testing system with small electromagnetic motors as the driving core;
◆ Meet the strict requirements of material mechanics testing for high-precision, high-frequency, high stability, and durability in biological material mechanics experiments;
◆ Optional torsion channel for multi axis tension and torsion loading;
◆ Can perform tests such as stretching, compression, bending, shearing, twisting (optional), creep, relaxation, etc;
◆ Suitable for testing metal materials, microelectronic materials, polymer materials, and biomaterials;
Multiple fixtures and accessories are available for selection.
Specification:
Axial loading | Maximum peak load | 100N |
Peak value of dynamic load | 100N | |
Peak value of static load | 40N | |
Load measurement range | 0.4%~100%F.S. | |
Load measurement accuracy | Better than ± 0.2% of the indicated value (within the load measurement range) | |
Maximum fatigue loading frequency | 100Hz | |
Axial travel | 40mm | |
Displacement resolution | 0.1μm | |
Torsion | Twisted loading form | Top mounted (pull/twist integrated) |
Dynamic peak torque | 5N·m | |
Torque measurement range | 0.4%~100%F.S. | |
Accuracy of torque measurement | Better than ± 0.2% of the indicated value (within the torque measurement range) | |
Maximum torsional loading frequency | 1Hz (static or low-frequency dynamic) | |
Angle measurement range | No angle limitation | |
maximum speed | 30r/min | |
Corner resolution | 0.018° | |
Test space (upper and lower clamp space) | 0-300mm | |
net weight | 75kg | |
External dimensions | 400×250×1200(mm) | |
Electrical requirements | AC220V 300W | |
Optional accessories | Bone nail fixture, clamp fixture, compression fixture, three-point bending fixture, etc | |
application | Static/dynamic testing of surgical implants (such as self tapping test, screw in/out test, low load static test, dynamic fatigue test, etc.) | |