ASTM F1264 Intramedullary Fixation Device Torsion & Bend Fatigue Testing Equipment
The UTDS series Dynamic/Fatigue Testing machine used for bone needle, bending intramedullary nail fatigue test is mainly used for biomechanical performance testing of various materials, including artificial blood vessels, soft tissues, bones, bone plates, and vertebrae Interfusion device, knee joint, spine Dynamic and static mechanical tests on materials such as column fixators, metal coatings, hip joints, and intramedullary nails, including tension, compression, bending, and torsion.
ASTM F1264 is a standard specification used to describe the design and mechanical function of intramedullary fixation devices (IMFDs). This specification covers IMFDs used for surgical fixation of the skeletal system. In addition to classification, terminology, labeling, and material specifications, it also includes four standard testing methods:
1, static four point bending test method (Annex A1),
2, static torsion test method (Annex A2),
3, bending fatigue test method (Annex A3),
4, bending fatigue test method for IMFD locking screws (Annex A4).
Main Parameter of the fatigue test machine:
Max. dynamic load: ±10KN Accuracy ±1%
Max. static load: ±10kN
Dynamic fluctuation: Less than ±1%FS
Actuator max. stroke: ±50mm, accuracy ±0.5%FS
Amplitude at Max. frequency: ±1mm
Max. Frequency: 0.1HZ~15Hz
Max. line velocity: 150mm/s
For more information or details, please contact us:
Email: export@unitedtest.com
whatsapp: +8613911165373
Max. dynamic load | ±10KN Accuracy ±1% |
Max. static load | ±10kN |
Dynamic fluctuation | Less than ±1%FS |
Actuator max. stroke | ±50mm, accuracy ±0.5%FS |
Amplitude at Max. frequency | ±1mm |
Max. Frequency | 0.1HZ~15Hz |
Max. line velocity | 150mm/s |
Control mode | Load, displacement, deformation |
Main test waveform | Sinusoidal wave, triangular wave, square wave, sawtooth wave etc., |
Pass through Zero | Complete display the pass through zero hysteresis loop curve. |
Columns number | 2 |
Vertical space | 750mm |
Max. test space | 450mm (include test fixture) |
Test width | 450mm |
Cooling method | Water cooling |
Weight | 350kg |
Dimensions | 785*620*2050mm |
Standard Power | 380/220V, 50/60HZ, 3 phase, 4Kw |
Working system | MS Win7 / Win10 |
Load cell | USA, Vishay Celtron |
ASTM F1264-16e1 Standard Specification and Test Methods for Intramedullary Fixation Devices
1.4 includes four standard test methods:
1.4.1 Static Four-Point Bend Test Method—Annex A1 and
1.4.2 Static Torsion Test Method—Annex A2.
1.4.3 Bending Fatigue Test Method—Annex A3.
1.4.4 Test Method for Bending Fatigue of IMFD Locking Screws—Annex A4.