ISO 7231 Polymeric materials, cellular, flexible — Determination of air flow value at constant pressure-drop 


ISO 7231 test standard specifies two methods for determining the air flow value of flexible cellular polymeric materials:

—     method A, for conventional types of flexible cellular polymeric material;

—     method B, for all types of flexible cellular polymeric material, but especially for materials with a low permeability to air.

For method B, two methods are specified in this document:

—     method B1: with manual measurement;

—     method B2: with automatic measurement.


NOTE 1       Air flow values can be used to give an indication of the effects of formulation and production variables on the cellular structure.

NOTE 2       In this document, the expression “conventional type of flexible cellular polymeric material” means types which are unsuitable for sealing purposes.


< Previous: ISO 7206-10 Femoral Head Static Compression and Tensile test

> Next: ISO 7438 Metallic materials Bending test details

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.