ISO 6964:2019 Polyolefin pipes and fittings — Determination of carbon black content by calcination and pyrolysis — Test method
This standard specifies test methods for the determination of the carbon black content of polyolefin compositions used in particular for the manufacture of pipes and fittings, and provides a basic specification for polyethylene pipes and fittings. ISO 6964 applies equally to the material for manufacture and to any material taken from a pipe or fitting.