Home >> Application >> By Standard >> ISO >> ISO 5000~9999 >> ISO 6308 Testing for Gypsum plasterboard Products

ISO 6308 Testing for Gypsum plasterboard Products

Share:

ISO 6308 Testing of Gypsum plasterboard Products


Relates to gypsum plasterboard intended to be used as a vertical or horizontal lining in buildings, excluding that which has been subjected to secondary manufacturing operations. Includes boards manufactured to receive either direct surface decoration or gypsum plaster finishes. Specifies the general characteristics of the boards and appropriate test methods and defines types and their various applications.


The test methos appear in the following order: 

(1) flexural strength (Method A); 

(2) core, end, and edge hardness (Method A); 

(3) nail pull resistance (Method A); 

(4) humidified deflection; 

(5) end squareness; 

(10) water resistance of core-treated water repellant gypsum panel products;

(11) surface water resistance of gypsum panel products with water-repellant surfaces.

< Previous: ISO 6259-3 Tensile test for Thermoplastics Polyolefin pipes

> Next: ISO 6475 Bone Screw Torsion Breaking Torque Test Methods

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.