ISO 13938-1 Textiles fabrics hydraulic bursting strength and bursting distension

Share:

ISO 13938-1:2019 Textiles — Bursting properties of fabrics — Part 1: Hydraulic method for determination of bursting strength and bursting distension


The method is applicable to knitted, woven, nonwoven and laminated fabrics. It can be suitable for fabrics produced by other techniques. The test is suitable for test specimens in the conditioned or wet state.


From the available data, there appears to be no significant difference in the bursting strength results achieved using hydraulic or pneumatic burst testers, for pressures up to 800 kPa. This pressure range covers the majority of performance levels expected of general apparel. For speciality textiles requiring high bursting pressures, the hydraulic apparatus is more suitable. 

ISO 13938-1 Textiles fabrics hydraulic bursting strength and bursting distension

< Previous: ISO 13937-1 Fabric and textiles Tearing test by Pendulum Elmendorf method

> Next: ISO 14125 Three points bending test of Fiber-Reinforced Plastic Composites

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.