ISO 11058 Geotextile water permeability test

Share:

ISO 11058 test specifies two test methods for the water permeability characteristics of a single layer of geotextile or geotextile-related product normal to the plane: the constant head method; and the falling head method.

ISO 11058:2019 Geotextiles and geotextile-related products — Determination of water permeability characteristics normal to the plane, without load. 


Water Flow through a Geotextile: Measuring Perpendicular Water Flow and Permittivity


ISO 11058 test standard specification discusses the methods for measuring water flow through geotextiles in the laboratory. This is an important characteristic, as it may be a crucial factor in determining the suitability of geotextiles for filtration, such as water flow into drainage layers. The main testing methods are 'vertical water flow' and 'permeability', which are similar but not identical. Broader information regarding the behavior of filter geotextiles is included in the technical specification titled 'Geotextile Filtration'. The vertical water flow measurement method, which measures vertical water flow (i.e., water flow perpendicular to the plane), is defined by EN ISO 11058, which is almost identical to ASTM D4491. 


The difference is that vertical water flow is defined as the flow rate (in liters per second) divided by the area of the geotextile being tested, but not divided by the head of water. EN ISO 11058 also uses a water head of 50mm for testing, and the results are expressed in velocity.


< Previous: ISO 11003-2 Thick-Adherend Tensile Shear Test for Structural Adhesives

> Next: ISO 11173 Plastic pipe falling weight impact test

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.