Home >> Application >> By Standard >> ISO >> ISO 10000~19999 >> ISO 10618 Carbon fibre tensile test of resin-impregnated yarn

ISO 10618 Carbon fibre tensile test of resin-impregnated yarn

Share:

ISO 10618:2004 Carbon fibre — tensile properties of resin-impregnated yarn

ISO 10618 specifies a method of test for the determination of the tensile strength, tensile modulus of elasticity and strain at maximum load of a resin-impregnated yarn specimen. The method is applicable to yarns (continuous and staple-fibre yarns) of carbon fibre for use as reinforcements in composite materials.

ISO 10618 Carbon fibre tensile test of resin-impregnated yarn

The test sample length: 250mm or 300mm without reinforced piece. 

If add the reinforced piece, the sample is 150mm or 200mm.  


UNITEDTEST supply the tensile testing machine to do this tensile property test. 

< Previous: ISO 10319 Geotextile Wide Width Strip tensile testing

> Next: ISO 11058 Geotextile water permeability test

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.