Home >> Application >> By Standard >> ISO >> ISO 10000~19999 >> ISO 10123 Determination of shear strength of anaerobic adhesives using pin-and-collar specimens

ISO 10123 Determination of shear strength of anaerobic adhesives using pin-and-collar specimens

Share:

ISO 10123:2013 Adhesives — Determination of shear strength of anaerobic adhesives using pin-and-collar specimens


ISO 10123 applies to anaerobic curing liquid adhesives used for locking and sealing threaded fasteners and to other adhesives. These adhesives cure without being dependent on exposed air. ISO 10123 defines a test method to assess this material in a way that is similar to the shear stresses that threads are exposed to in their regular environment, but with defined surface areas to make shear strength calculations straightforward. The common name of this technique is the pin-and-collar method. 

ISO 10123 Determination of shear strength of anaerobic adhesives using pin-and-collar specimensISO 10123 Determination of shear strength of anaerobic adhesives using pin-and-collar specimens


Related Standard

ISO 29862 Tape adhesion peeling test, Self adhesive tapes –

ISO 29862 Self adhesive tapes — Determination of peel adhesion properties

ISO 29862 specifies peel adhesion force of pressure-sensitive adhesive (PSA) tapes under controlled laboratory conditions. It covers four core 180° peel test methods plus two normative annexes for low-temperature and 90° peel testing, serving as a universal quality control and material comparison benchmark for adhesive tape manufacturers, laboratories and end users worldwide.

ISO 8510-2 Adhesives 180 degree peel test for flexible-bonded-to-rigid test specimen assembly –

ISO 8510-2: Adhesives — Peel test for a flexible-bonded-to-rigid test specimen assembly Part 2: 180° peel.

ISO 8510-2 specifies a 180° peel test for determining the peel resistance of a bonded assembly where one adherend is flexible and the other is rigid. Measures the peel resistance of structural liquid adhesive bonds where one adherend is flexible and the other rigid. It only applies to cured structural adhesives (epoxy, PU, wood glue, contact adhesives) – not pressure-sensitive adhesive tapes. It provides repeatable comparative peel force data for R&D, factory quality control, supplier qualification and commercial dispute resolution.

ISO 11339 T-peel test for Adhesives –

ISO 11339 Adhesives — T-peel test for flexible-to-flexible bonded assemblies.

It specifies a T‑peel test for the determination of the peel resistance of an adhesive by measuring the peeling force of a T‑shaped bonded assembly of two flexible adherends.  The ISO 11339 test method is suitable for self-adhesive tapes that are prepared under the relevant guidelines within this test standard. For a T-peel test for a flexible-to-flexible assembly, the force is applied to the unbonded ends of the specimen . The angle between the bond line and the direction of the applied force is not fixed. 

< Previous: None

> Next: ISO 10191 Passenger Car Tyre Test - Endurance, High-Speed, Bead unseating