ISO 4422-2 Pipes and fittings made of PVC-U for water supply

Share:

ISO 4422-2:1996Pipes and fittings made of unplasticized poly (vinyl chloride) (PVC-U) for water supply - Specifications - Part 2: Pipes (with or without integral sockets). 

ISO 4422-2 specifies the characteristics and properties of extruded pipes made of unplasticized poly (vinyl chloride) (PVC-U), with or without socket(s) (integral or not), intended to be used for buried water mains and services and for water suppliers above ground, both inside and outside buildings.

< Previous: ISO 4152 Beam Bending Measure Apparent Axial Long Term Modulus of GRP Pipes

> Next: ISO 4437-1 Tensile, Hydrostatic pressure test for Plastics PE piping systems for the supply of gaseous fuels

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.