Home >> Products >> Industrial Specialized Testing >> Civil Engineering

Civil Engineering

In the construction engineering and building materials industry, mechanical testing determines the compressive and tensile properties of materials such as concrete and steel, which is core to ensuring the safety and durability of buildings. UnitedTest can cover the full range of building material mechanical tests, complies with ISO, ASTM international standards, and provides customized testing solutions for compressive, tensile, and other properties.

Feature:

  • Comparable with the Schmidt Hammer, Type N
  • EN 12 504-2, ASTMC805, DIN 1048 and BS1881 part 202

Key parameter:

  • Measuring ranges: 10-70MPa
  • Impact energy: 2.207J (0.225Kgf.m)
  • Spring extension: 75±0.3mm
Details

Feature:

  • Dual control method allows operation through the touchscreen or via a computer
  • Burners can automatically rotate.

Key parameter:

  • Smoke density measurement range: 0~100%
  • measurement accuracy: ±3%
  • Main burner working pressure: 276KPa
Details

Feature:

  • Fully automated measurement.
  • Can tests 8 samples same time.
  • Can add samples for tests at any time.

Key parameter:

  • Linear displacement measurement accuracy: ≤50µm
  • Max. 8 test samples
  • Effective length of test needle: 70±1mm
Details

Feature:

  • Fully automated measurement.
  • Can tests 8 samples same time.
  • Can add samples for tests at any time.

Key parameter:

  • Linear displacement measurement accuracy: ≤50µm
  • Max. 8 test samples
  • Effective length of test needle: 70±1mm
Details

Feature:

  • One-key operation of position calibration
  • Automation of the measurement process
  • Support RS485 interface data output

Key parameter:

  • Sliding component: 300g±1g
  • Displacement: 50mm
  • display precision: 0.01s
Details

Feature:

  • Color touch screen display

Key parameter:

  • Measurement range: 0 to 3.0 MPa
  • Resolution: 0.001 MPa
  • Specimen size: no less than 55 mm
Details

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now