Home >> Application >> By Standard >> ASTM >> ASTM E-F >> ASTM F1160 Shear and Bending Fatigue testing of Coatings for Calcium Phosphate and Metallic

ASTM F1160 Shear and Bending Fatigue testing of Coatings for Calcium Phosphate and Metallic

Share:

ASTM F1160 Standard Test Method for Shear and Bending Fatigue Testing of Calcium Phosphate and Metallic Medical and Composite Calcium Phosphate/Metallic Coatings;


Rotating beam fatigue testing generates higher frequencies than traditional high cycle fatigue (HCF) methods. UnitedTest testing services provide critical data about coatings and metallic surface treatments to ISO 1143, ASTM F1160 standards. 


Rotating beam fatigue testing, Shear and Bending Fatigue testing. 

Rotating beam fatigue testing is a mechanical test method used to evaluate the fatigue properties of materials. In this test, a beam specimen is subjected to cyclic loading, which induces repeated bending causing failure over time. The specimen is mounted on a rotating apparatus, which allows for the cyclic load to be applied at constant amplitude and frequency.

During the test, the beam specimen is rotated at a constant speed while a loading force is applied to it. The force causes the beam to bend, and as the beam rotates, it undergoes cyclic bending stress that can induce fatigue failure.

The data generated can be used to design and optimize materials for use in applications where fatigue failure is a concern, such as the Aerospace and Automotive industries.

Shear and bend fatigue testing determines the coating's adhesive or cohesive properties. Bend fatigue testing also provides information on the effects of the coating on the metallic substrate.

ASTM F1160 Shear and Bending Fatigue testing of Coatings for Calcium Phosphate and Metallic

ASTM F1160 Equipment and Sample Preparation

Specimen Details: The ASTM F1160 specimens used are calcium phosphate metallic, or composite coatings containing calcium phosphate and metallic layers.

Specimen dimensions: The acceptable specimen size varies with the testing requirements.

Specimen Preparation: The ASTM F1160 specimens are cleaned and prepared as per requirements.

Related products and device

ASTM F1160 shear test fixture

Coating static shear strength testing refers to ASTM F1044, F1160 standard, evaluating the shear force of continuous calcium phosphate coating or metal coating on the substrate, or the bonding strength between coatings parallel to the horizontal plane after shearing.

Related Standard

ASTM F2068 Fatigue test system of Femoral Prostheses Implants, Hip Implants Testing –

ASTM F2068: Standard Specification for Femoral Prostheses – Metallic Implants


ASTM F2068 covers metallic stemmed femoral prostheses used to replace the natural hip joint by means of hemi-arthroplasty or total hip surgical procedures. Prostheses for hemi-arthroplasty are intended to articulate with the natural acetabulum of the patient. Prostheses for total hip replacement are intended to articulate with prosthetic acetabular cups. Prostheses may have integral femoral heads or cones designed to accept modular heads. 

The mechanical strength (fatigue test ISO 7206-4, ISO 7206-6, shear strength test ASTM F1044, tensile test ASTM F1147, abrasion resistance test ASTM F1978), corrosion resistance, and biocompatibility of the head portions of one-piece integral implants are covered by this specification.

ISO 1143 Rotating bar bending fatigue test by rotating rod bending –

ISO 1143:2021 is a standard for fatigue testing of metal materials by rotating rod bending, which specifies in detail how to design and perform rotating rod bending fatigue tests to evaluate the fatigue performance of metal materials.


Test objective: To evaluate the fatigue performance of metal materials under rotational bending conditions.

Scope of application: Suitable for various metal materials, including steel, aluminum alloys, etc. Testing principle: The specimen is rotated at a specified speed and subjected to bending load on the testing machine until it fractures or reaches the preset number of cycles.

This standard provides a detailed description of the construction and operation methods of testing equipment, including rotary bending testing machines, specimen fixtures, loading systems, and measurement systems.

< Previous: ASTM F1147 Tension Testing for Calcium Phosphate and Metallic Coatings

> Next: ASTM F1264 Intramedullary Fixation Device Torsion & Bend Fatigue Test

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.