Home >> Application >> By Standard >> ASTM >> ASTM D >> ASTM D3895 Oxidative-Induction Time Test by Differential Scanning Calorimetry

ASTM D3895 Oxidative-Induction Time Test by Differential Scanning Calorimetry

Share:

ASTM D3895: Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry.


ASTM D3895 test method outlines a procedure for the determination of oxidative-induction time (OIT) of polymeric materials by differential scanning calorimetry (DSC). It is applicable to polyolefin resins that are in a fully stabilized/compounded form.


Significance and Use:

1 The oxidative induction time is a characteristic of a compounded polyolefin product that is dependent not only on the type and amount of additives present, but also on the type of resin. In well-behaved systems, this test method can be used as a quality control measure to monitor the stabilization in geosynthetics as received from a supplier.

2 When this test method is used to compare different geomembrane formulations containing different antioxidant packages, then those results shall be considered valid only at the temperature of test.

3 This test method is intended as a geosynthetic test. Use of the OIT value to estimate the lifetime of the geomembrane from which the test specimen is taken is not addressed, nor shall it be used for this purpose.

Caution should be exercised in data interpretation since oxidation reaction kinetics are a function of temperature and the properties of the additives contained in the geosynthetic sample. For example, OIT values are often used to select optimum resin formulations. Certain antioxidants, however, may generate poor OIT results even though they may be adequate at their intended use temperature and vice versa.

ASTM D3895 Oxidative-Induction Time Test by Differential Scanning Calorimetry

Related standard:

ASTM D5885/D5885M: Standard Test Method for Oxidative Induction Time of Polyolefin Geosynthetics by High-Pressure Differential Scanning Calorimetry.

ASTM D8117: Standard Test Method for Oxidative Induction Time of Polyolefin Geosynthetics by Differential Scanning Calorimetry.

Related Standard

ISO 1133 Test Method of Determination melt mass-flow rate (MFR, MVR) –

ISO 1133: Plastics -- Determination of the melt mass-flow rate (MFR) and the melt volume-flow rate (MVR) of thermoplastics.

ISO 1133 standard specifies two procedures for the determination of the melt mass-flow rate (MFR) and the melt volume-flow rate (MVR) of thermoplastic materials under specified conditions of temperature and load. One is a mass-measurement method. The other is a displacement-measurement method. Normally, the test conditions for measurement of melt flow rate are specified in the material standard with a reference to ISO 1133. The test conditions normally used for thermoplastics are listed in annexes. 

< Previous: ASTM D3787 Textile Ball Burst Constant Rate Traverse CRT Test

> Next: ASTM D3999 Soil Secant Modulus and Damping Coefficient by Dynamic Cyclic Triaxial Testing