Home >> Application >> By Standard >> ASTM >> ASTM D >> ASTM D2466 PVC Plastic Pipe fitting burst test method

ASTM D2466 PVC Plastic Pipe fitting burst test method

Share:

ASTM D2466: Standard Specification for Poly(Vinyl Chloride) (PVC) Plastic Pipe Fittings, Schedule 40

ASTM D2466 test covers poly(vinyl chloride) (PVC) Schedule 40 pipe fittings. Included are requirements for materials, workmanship, dimensions, and burst pressure. the products covered by this specification are intended for use with the distribution of pressurized liquids only, which are chemically compatible with the piping materials. Fitting such as unions, flanges, special plastic-to-metal transitions and appurtenances intended for use with PVC piping are covered under Specification ASTM F1970.

ASTM D2466 PVC Plastic Pipe fitting burst test method


ASTM D2466 PVC Plastic Pipe Fittings burst pressure test fixture made by UnitedTest:

ASTM D2466 PVC Plastic Pipe fitting burst test method


Related standard: 

ASTM D2672: Standard Specification for Joints for IPS PVC Pipe Using Solvent Cement

ASTM F441: Standard Specification for Chlorinated Poly(Vinyl Chloride) (CPVC) Plastic Pipe, Schedules 40 and 80

ASTM F442: Standard Specification for Chlorinated Poly(Vinyl Chloride) (CPVC) Plastic Pipe (SDR–PR)

< Previous: ASTM D2444 Pipe falling weight impact test standard

> Next: ASTM D2565 Xenon Arc Aging Test of Plastics

Require More Customized Solutions?

We offer customization to meet your specific needs. Our expert team will collaborate with you to develop the perfect product for you
Customize Now

Beijing United Test Co., Ltd.